Takaitaccen Bayani:

A902 (AWS E320-16) wani lantarki ne na bakin karfe wanda ke da rufin titanium-calcium. Ana iya amfani da shi don AC da DC tare da kyakkyawan aikin aiki.


Cikakken Bayani game da Samfurin

Alamun Samfura

Walda Bakin KarfeElektrode

A902

GB/T E320-16

AWS A5.4 E320-16

Bayani: A902 wani lantarki ne na bakin karfe wanda ke da rufin titanium-calcium. Ana iya amfani da shi don AC da DC tare da kyakkyawan aikin aiki. Karfe da aka ajiye yana da kyakkyawan juriya ga tsatsa da juriya ga iskar shaka kuma ana amfani da shi sosai wajen kera masana'antar sinadarai, man fetur, da kayan aikin samar da hydrogen.

Aikace-aikace: Ana amfani da shi don walda ƙarfe mai ƙarfe mai kama da Carpenter20Cb a cikin sinadarin sulfuric acid, nitric acid, phosphoric acid da kuma sinadarin oxidative acid. Haka kuma ana iya amfani da shi don walda ƙarfe daban-daban.

 

Sinadarin sinadarai na ƙarfen walda(%):

C

Si

Mn

Cr

Ni

Mo

Cu

Nb

S

P

≤0.07

≤0.60

0.5 ~ 2.5

19.0 ~ 21.0

32.0 ~ 36.0

2.0 ~ 3.0

3.0 ~ 4.0

8 XC ~ 1.00

≤0.030

≤0.030

 

Kayan aikin injiniya na ƙarfe na walda:

Gwaji abu

 Ƙarfin tauri

Mpa

Ƙarawa

%

An Garanti

≥550

≥30

 

Shawarar da ake bayarwa:

Diamita na sanda

(mm)

2.5

3.2

4.0

Walda na Wuta

(A)

50 ~ 80

80 ~ 110

110 ~ 160

 

Sanarwa:

  1. Dole ne a gasa wutar lantarki na tsawon awa 1 a kusan 150℃ kafin a fara aikin walda;
  2. Saboda zurfin shigar ciki ba shi da zurfi yayin walda ta AC, ya kamata a yi amfani da wutar lantarki ta DC gwargwadon iyawa don samun zurfin shigar ciki. Kuma kada wutar ta yi girma sosai don guje wa jajayen sandar walda.

 

 

An kafa Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun kasance muna ƙerana'urar waldas, sandunan walda, kumaabubuwan da ake amfani da su na waldasama da shekaru 20.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 


  • Na baya:
  • Na gaba: