AWS E2209-16 Bakin Karfe Welding Sanduna, Bakin Karfe rufe Electrode Filler Sanduna

Takaitaccen Bayani:

AF2209-16 (AWS E2209-16) ultra-low carbon nitrogen-dauke da duplex bakin karfe lantarki tare da titanium-calcium shafi.


Cikakken Bayani

Tags samfurin

Bakin Karfe WeldingElectrode

Saukewa: AF2209-16                               

GB/T E2209-16

AWS A5.4 E2209-16

Bayani: AF2209-16 ultra-low carbon nitrogen-dauke da duplex bakin karfe lantarki tare da titanium-calcium shafi.Ana iya amfani dashi don duka AC da DC tare da kyakkyawan aikin aiki.Domin yana dauke da molybdenum da nitrogen, kuma abun da ke cikin carbon din ya yi kasa sosai, karfen da aka ajiye yana da kyakykyawan juriya na tsagewa da juriya, musamman juriyar lalatawar danniya.

Aikace-aikace: An yafi amfani da waldi iri ɗaya nau'in ultra-low carbon bakin karfe kayan a cikin man fetur da kuma na'ura mai aiki da karfin ruwa masana'antu.Kamar waldi na 022Cr22Ni5Mo3N duplex bakin karfe.

 

Abubuwan sinadaran na weld karfe(%):

C

Mn

Si

Cr

Ni

Mo

N

Cu

S

P

≤0.04

0.5 ~ 2.0

≤0.90

21.5 ~ 23.5

8.5 ~ 10.5

2.5 ~ 3.5

0.08 ~ 0.20

≤0.75

≤0.030

≤0.040

 

Abubuwan kayan aikin walda:

Gwaji abu

Ƙarfin ƙarfi

Mpa

Tsawaitawa

%

Garanti

≥ 690

≥20

 

Shawarwari na yanzu:

Diamita na sanda

(mm) da

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 70

80 ~ 110

130 ~ 150

160 ~ 200

 

Sanarwa:

1. Dole ne a gasa wutar lantarki don 1 hour a kusa da 250 ℃ kafin aikin walda;

2. Yana da mahimmanci don tsaftace tsatsa, sikelin mai, ruwa, da ƙazanta akan sassan walda kafin walda.

 

 

Wenzhou Tianyu Electronic Co., Ltd. da aka kafa a 2000. Mun aka tsunduma a cikin masana'antu nawalda lantarkis, sandunan walda, kumaabubuwan amfani da waldafiye da shekaru 20.

Babban samfuranmu sun haɗa da bakin karfewalda lantarkis, carbon karfe walda lantarki, low gami waldi lantarki, surfacing waldi lantarki, nickel & cobalt gami waldi lantarki, m karfe & low gami waldi wayoyi, bakin karfe walda wayoyi, gas-garre juyi cored wayoyi, aluminum walda wayoyi, submerged baka waldi .wayoyi, nickel & cobalt alloy walda wayoyi, tagulla walda wayoyi, TIG & MIG walda wayoyi, tungsten electrodes, carbon gouging lantarki, da sauran walda na'urorin & consumables.

 

 


  • Na baya:
  • Na gaba: