Nickel Alloy Welding Wire ERNi-1 Nickel Tig Wire Filler Metal

Takaitaccen Bayani:

Ana amfani da ER-Ni1 don waldawa da walƙiya na nickel 200 da nickel 201 gami.


Cikakken Bayani

Tags samfurin

Nickel AlloyWaya WeldingTig WayaERNi-1

Matsayi
TS EN ISO 18274 - Ni 2061 - NiTi3
AWS A5.14 - ER Ni-1

 

Fasaloli da Aikace-aikace

Ana amfani da ER-Ni1 don waldawa da walƙiya na nickel 200 da nickel 201 gami.

Cikakke don haɗa Monel gami da jan ƙarfe-nickelalloys zuwa carbon steels.

Ni1 ya ƙunshi isassun titanium don sarrafa porosity na weld-karfe akan hanyoyin walda.

Yawanci ana amfani dashi a masana'antar sarrafa sinadarai, samar da fiber na roba & kayan sarrafa abinci da dai sauransu.

 

Kayayyakin Tushe Na Musamman

Nickel 200 da 201*
* Misali, ba cikakken lissafi ba

 

Haɗin Sinadari%
C% Mn% Fe% P% S% Si%  
max max max max max max  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Ku% Ni% Co% Ti% Al%    
max 93.00 max 2.00 max    
0.20 min 1.00 3.50 1.00    

 

Kayayyakin Injini
Ƙarfin Ƙarfin Ƙarfi ≥410 MPa  
Ƙarfin Haɓaka ≥200 MPa  
Tsawaitawa ≥30%  
Ƙarfin Tasiri ≥ 100 J  

Kaddarorin injina sun yi kusan kuma suna iya bambanta dangane da zafi, gas ɗin kariya, sigogin walda da sauran abubuwa.

 

Garkuwar Gas

TS EN ISO 14175 TIG: I1 (Argon)

 

Matsayin walda

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Bayanan tattara bayanai
Diamita Tsawon Nauyi  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 kg

5 kg

 

 

Alhaki: Duk da yake an yi duk ƙoƙarin da ya dace don tabbatar da daidaiton bayanan da ke ƙunshe, wannan bayanin yana iya canzawa ba tare da sanarwa ba kuma ana iya ɗaukarsa azaman dacewa da jagora gabaɗaya.