GB/T EZNiCu-1 (Z508) Cast Iron Welding Electrode Nickel-Copper Alloy (Monel) Core and Graphitized Coating

Takaitaccen Bayani:

GB/T EZNiCu-1 (Z508) simintin gyare-gyaren ƙarfe ne na ƙarfe mai walƙiya tare da core nickel-Copper gami (Monel) da kuma shafi mai zane.


Cikakken Bayani

Tags samfurin

Cast Iron WeldingElectrode

Z508                                                     

GB/T EZNiCu-1

Bayani: Z508 simintin ƙarfe ne na waldawa lantarki tare da ginshiƙi na nickel-Copper Alloy (Monel) da shafi mai graphitized.AC da DC dual-manufa, barga baka, mai sauƙin aiki.Ƙirƙirar aikinta da aikin yankewa yana kusa da Z308, amma saboda girman raguwar ƙarfe da aka ajiye, juriyar tsaga ba ta da kyau.Ƙarfin haɗin gwiwar welded yana da ƙasa, don haka bai dace da walda na sassa masu damuwa ba.

Aikace-aikace: Ana amfani da shi don gyaran walda na simintin ƙarfe mai launin toka wanda baya buƙatar ƙarfin ƙarfi.

 

Abubuwan sinadaran na weld karfe(%):

C

Si

Mn

Fe

S

Ni

Cu

Wasu

0.35 ~ 0.55

≤0.75

≤2.3

3.0 ~ 6.0

≤0.025

60 ~ 70

25 ~ 35

≤1.0

 

Shawarwari na yanzu:

Diamita na sanda

(mm) da

3.2

4.0

5.0

Welding halin yanzu

(A)

90 ~ 110

120 ~ 150

160 ~ 190

 

Sanarwa:

1. A lantarki dole ne a gasa ga 1 hour a kusa da 150 ℃ kafin walda aiki;

2. Lokacin waldawa, yana da kyau a yi amfani da kunkuntar hanya, kuma tsawon kowane weld kada ya wuce 50mm.Nan da nan yi guduma weld ɗin da ƙaramin guduma don rage damuwa a wurin gyaran walda da hana fasa bayan walda.

 

 

Wenzhou Tianyu Electronic Co., Ltd. da aka kafa a 2000. An tsunduma a cikin masana'antu na walda lantarki, waldi sanduna, da kumawaldi mai amfanis fiye da shekaru 20.

Babban samfuranmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walƙiya na carbon karfe, ƙananan lantarki waldi na lantarki, lantarki waldi na walƙiya, nickel & cobalt alloy walda lantarki, ƙananan ƙarfe & ƙananan wayoyi masu walƙiya, bakin karfe walƙiya wayoyi, gas-garkuwar juzu'i cored wayoyi, aluminum walda wayoyi, nutsewar baka waldi.wayoyi, nickel & cobalt alloy walda wayoyi, tagulla walda wayoyi, TIG & MIG walda wayoyi, tungsten electrodes, carbon gouging lantarki, da sauran walda na'urorin & consumables.

 


  • Na baya:
  • Na gaba: