AWS A5.4 E309L-16 Bakin Karfe Welding Sanduna Mafi kyawun Welding Electrode

Takaitaccen Bayani:

A062 (AWS E309L-16) wani ultra-low carbon Cr23Ni13 bakin karfe lantarki tare da titanium-calcium shafi.


Cikakken Bayani

Tags samfurin

Bakin Karfe Welding Electrode

A062                                         

GB/T E309L-16

Saukewa: E309L-16

Bayani: A062 ultra-low carbon Cr23Ni13 bakin karfe lantarki tare da titanium-calcium shafi.Ana iya amfani da shi duka biyu AC da DC.Yana da ƙananan abun ciki na carbon, don haka zai iya tsayayya da lalata intergranular da hazo na carbide ke haifar ba tare da stabilizers kamar niobium da titanium ba.

Aikace-aikace: Ana amfani da shi don nau'in nau'in nau'in ƙarfe na ƙarfe, ƙarfe mai haɗaka, da kayan haɗin ƙarfe na musamman a cikin kera fiber na roba, petrochemical, da sauran kayan aiki.Hakanan za'a iya amfani da shi don hawan matakan mika mulki a bangon ciki na tasoshin matsin lamba na makamashin nukiliya da walda na na'urorin hasumiya.

 

Abubuwan sinadaran na weld karfe(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.04

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

≤0.75

≤0.75

≤0.030

≤0.040

 

Abubuwan kayan aikin walda:

Gwaji abu

Ƙarfin ƙarfi

Mpa

Tsawaitawa

%

Garanti

≥520

≥25

 

Shawarwari na yanzu:

Diamita na sanda

(mm) da

2.5

3.2

4.0

5.0

Welding Current

(A)

50 ~ 70

80 ~ 110

130 ~ 160

160 ~ 200

 

Sanarwa:

1. Dole ne a gasa wutar lantarki don 1 hour a kusa da 150 ℃ kafin aikin walda;

2. Saboda zurfin shigar ciki ba shi da zurfi a lokacin waldi na AC, ya kamata a yi amfani da wutar lantarki ta DC gwargwadon yadda zai yiwu don samun zurfin shigar ciki.kuma kada na yanzu ya zama babba don gujewa jajayen sandar walda

 

An kafa Wenzhou Tianyu Electronic Co., Ltd a shekara ta 2000. Mun tsunduma a cikin masana'antu na walda lantarki, walda sanduna, da walda consumable fiye da shekaru 20.

Babban samfuranmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walƙiya na carbon karfe, ƙananan lantarki waldi na lantarki, lantarki waldi na walƙiya, nickel & cobalt alloy walda lantarki, ƙananan ƙarfe & ƙananan wayoyi masu walƙiya, bakin karfe walƙiya wayoyi, gas-garkuwar juzu'i cored wayoyi, aluminum walda wayoyi, nutsewar baka waldi.wayoyi, nickel & cobalt alloy walda wayoyi, tagulla walda wayoyi, TIG & MIG walda wayoyi, tungsten electrodes, carbon gouging lantarki, da sauran walda na'urorin & consumables.

OEM/ODM:

Muna goyan bayan OEM/ODM kuma muna iya yin marufi daidai da ƙirar ku, da fatan za a tuntuɓe mu don tattaunawa dalla-dalla.