AWS/ASME A 5.3 E 3003 Aluminum Welding Electrodes

Takaitaccen Bayani:

Don arc waldi aluminum gami da manganese da magnesium.Hakanan yana da kyau don haɗa nau'ikan nau'ikan aluminium da aikace-aikacen ruwan teku


Cikakken Bayani

Tags samfurin

Ƙarƙashin allo mai ɗimbin ɗigo huɗu, an ƙera shi da fari tare da firam ɗin zinare mai ƙwanƙwasa da lafazi, da madaidaicin gilashin da ke rufe saman saman.Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwararren Ƙwaƙwalwa na Ƙaƙwalwa na Ƙaƙwal na Ƙaƙwal na Ƙaƙwal na Ƙaƙwal na Ƙaƙwalwa na Ƙaƙƙi ) ya yi ga kowane wuri mai rai.Cikakke ga duk wanda ke sha'awar kayan daki masu salo da kayan marmari.

Tarin Gillmore Alberto ya dace don masu ƙirƙira kayan alatu & gidajen nuni.

Tare da tsaftataccen layukan zamani da kintsattse, dalla-dalla, kowane yanki (wani lokaci) abu ne mai tsayi don abubuwan ciki, wanda aka ƙera tare da amfani a zuciya.Duk kayan lacquered ana samun su a cikin satin matt fari ko matt launin toka, tare da kyakkyawan ƙarfe mai ƙayatarwa a cikin tagulla ko baƙin chrome don ɗaukar kyan gani na zamani tare da sha'awar duniya.

Ɗaya daga cikin fasalulluka na musamman a cikin wannan tarin shine saman gilashin da ya dace da shi don duk ɗakunan mu na Alberto don taɓawa mai ɗorewa na inganci mara kyau.Bugu da ƙari, ana samun zaɓuɓɓukan ajiya masu karimci, kamar yadda raka'a ke daidaitawa kuma ana isar da su cikin ingantattun abubuwan haɓaka don sauƙaƙe damuwa da ke zuwa tare da sufuri da shigarwa.


DIN: 1732: EL Si-Al Mn

SIFFOFI & APPLICATIONS:

Don arc waldi aluminum gami da manganese da magnesium.Hakanan yana da kyau don haɗa nau'ikan nau'ikan aluminium da aikace-aikacen ruwan teku.

Aluminum baka walda lantarki tare da keɓaɓɓen slag dagawa kai.Hakanan ana samun sauran nau'ikan aluminium kamar 12% Si, 5% Si da E 1100, da sauransu.

Slag ɗin dagawa na musamman.

Tsaftace farin dogon shiryayye rai extruded juriya shafi wuce al'ada kayayyakin a danshi juriya.

Ana iya ƙera su a cikin launuka na al'ada iri-iri.

Akwai a cikin gwangwani PURE ALUMINUM da aka rufe ta hanyar hermetically ko buhunan jakunkuna masu dumbin yawa don tsawan rayuwa.

DUKAN WELD KARFE ANALYSIS (nauyi na al'ada%):

Launi Flux: Fari ko Launi na Musamman

Si Cu Fe Zn Mn Be Zr Ti Al
0.14 .07 0.23 .002 1.3 .0001 .0004 .009 Bal.

KAYAN KYAUTA NA KANKANI:

Ƙarfe mara Diluted Weld Matsakaicin Ƙimar Har zuwa

Ƙarfin Tensile 34,000 psi (250 N/MPa)

Ƙarfin Haɓaka 20,000 psi (150 N/MPa)

Tsawaita 10%

WELDING NA YANZU & UMARNI:

Shawarar Yanzu: DC Reverse (+)
Diamita (mm) 3/32 (2.5) 1/8 (3.25)
Mafi ƙarancin Amperage 50 70
Matsakaicin Amperage 80 120

Dabarun walda: Fara da amfani da ɓangaren sama na kewayon amperage.Ciyar da lantarki da sauri kuma ka matsa cikin sauri tare da kiyaye tazarar baka na kusa.

Matsayin walda: Flat, Horizontal

MATSALAR ARZIKI:

Diamita (mm) Tsawon (mm) Weldmetal/Electrode Electrodesper lb (kg) na Weldmetal Lokacin Arc na Depositionmin/lb (kg) Saitunan Amperage Yawan farfadowa
3/32 (2.5) 14 ″ (350) .14oz (4.3g) 114 (251) 110 (242) 70 90%
1/8 (3.25) 14 ″ (350) .23oz (6.5g) 70 (153) 62 (136) 110 90%
5/32 (4.0) 14 ″ (350) .33oz (9.6g) 48 (107) 47 (103) 135 90%

KIMANIN CUTAR ELECTRODE & GIRMA:

Diamita (mm) 3/32 (2.5) 1/8 (3.25) 5/32 (4.0)
Tsawon (mm) 14 ″ (350) 14 ″ (350) 14 ″ (350)
Electrodes / lb 49 33 23
Electrodes / kg 108 73 51