Wayar Walda ta Nickel Alloy ERNiCrMo-3 Tig Waya

Takaitaccen Bayani:

ERNiCrMo-3 waya ce mai girman nickel wadda aka ƙera don walda da kuma rufe ƙarfe masu tushen nickel kamar 625 ko makamancin haka.


Cikakken Bayani game da Samfurin

Alamun Samfura

Alloy na NickelWayar WaldaWayar TigERNiCrMo-3

 

Fasaloli da Aikace-aikace

BabbannickelWayar ƙarfe da aka ƙera don walda da rufinnickel-based alloy kamar 625 ko makamancin haka.

An zana shi da ƙarfi ta hanya ta musamman don samun walda masu tsabta da inganci tare da dinki mai haske da kuma kyakkyawan aiki.

Ƙarfe mai walda yana da kyawawan halaye na injiniya a yanayin zafi mai zafi da ƙasa.

Kyakkyawan juriya ga tsatsa da kuma tsatsa.

Zafin aiki da aka ba da shawarar ya kama daga cryogenic zuwa 540°C.

Ana amfani da shi sosai a masana'antar sarrafa sinadarai, injiniyan ruwa, kayan aikin nukiliya, sararin samaniya da kuma a cikin kayan aikin sarrafa gurɓataccen iska da sauransu.

Kayan Tushe na Al'ada

Inconel 601, Incoloy 800, Alloy 625, Alloy 825, Alloy 926*
* Jerin misalai, ba cikakken bayani ba

 

Ma'auni
TS EN ISO 18274 - Ni 6625 - NiCr22Mo9Nb
AWS A5.14 – ER NiCrMo-3

 

Sinadarin Sinadarai %

C%

Mn%

Fe%

P%

S%

Si%

Ku%

matsakaicin

matsakaicin

matsakaicin

matsakaicin

matsakaicin

matsakaicin

matsakaicin

0.10

0.50

0.50

0.015

0.015

0.50

0.50

Ni%

Co%

Al%

Ti%

Cr%

Nb+Ta%

Mo%

60.00

matsakaicin

matsakaicin

matsakaicin

20.00

3.15

8.00

minti

1.0

0.40

0.40

23.00

4.15

10.00

 

Kayayyakin Inji
Ƙarfin Taurin Kai ≥760 MPa  
Ƙarfin Ba da Kyauta ≥415 MPa  
Ƙarawa ≥35%  
Ƙarfin Tasiri ≥100 J  

Kayayyakin injiniya suna da ƙima kuma suna iya bambanta dangane da zafi, iskar gas mai karewa, sigogin walda da sauran abubuwa.

 

Iskar Gas Mai Kariya

TS EN ISO 14175 TIG: I1 (Argon)

 

Wurare na Walda

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Bayanan Marufi
diamita Tsawon Nauyi  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 

Alhaki: Duk da cewa an yi duk mai yiwuwa don tabbatar da daidaiton bayanin da ke ciki, wannan bayanin yana iya canzawa ba tare da sanarwa ba kuma ana iya ɗaukarsa a matsayin wanda ya dace da jagora na gaba ɗaya.

 