Nickel Alloy Welding Waya ERNiCrMo-10 Tig Wire

Takaitaccen Bayani:

Nickel-chromium-molybdenum gami da aka ƙera don haɗawa da C22, 625, 825 ko haɗin waɗannan gami.


Cikakken Bayani

Tags samfurin

Nickel AlloyWaya WeldingTig WayaERNiCrMo-10

 

 

Matsayi
TS EN ISO 18274 - Ni 6022 - NiCr21Mo13Fe4W3
AWS A5.14 - ER NiCrMo-10

 

Fasaloli da Aikace-aikace

Nickel-chromium-molybdenum gami da aka ƙera don haɗawa da C22, 625, 825 ko haɗin waɗannan gami.

Yana ba da ƙaƙƙarfan ƙarfe mai walƙiya na Nb don walda iri ɗaya a cikin super austenitic da super duplex bakin karfe.

Yana ba da ingantacciyar juriya ga damuwa & lalata lalata, pitting da lalata ɓarna.

Ana amfani da shi sosai don overlays da cladding na ƙananan gami da karafa.

Yawanci ana amfani da shi a cikin walda na kafofin watsa labaru masu lalata a cikin masana'antar sarrafa sinadarai, lalata resistant overlays da kuma a cikin m teku da petrochemical muhallin da dai sauransu.

Ana iya samun takaddun shaida akan layi @wilkinsonstar247.com

Kayayyakin Tushe Na Musamman

Alloy 22, Alloy 625, Alloy 825, Alloy 926*
* Misali, ba cikakken lissafi ba

 

 

Haɗin Sinadari%

C%

Mn%

Fe%

P%

S%

Si%

Ku%

max

max

2.00

max

max

max

max

0.010

0.50

6.00

0.020

0.010

0.08

0.50

Ni%

Co%

Cr%

Mo%

V%

W%

49.00

max

20.00

12.50

max

2.50

min

2.50

22.50

14.50

0.30

3.50

Kayayyakin Injini
Ƙarfin Ƙarfin Ƙarfi ≥690 MPa
Ƙarfin Haɓaka -
Tsawaitawa -
Ƙarfin Tasiri -

Kaddarorin injina sun yi kusan kuma suna iya bambanta dangane da zafi, gas ɗin kariya, sigogin walda da sauran abubuwa.

 

Garkuwar Gas

TS EN ISO 14175 TIG: I1 (Argon)

 

Matsayin walda

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Bayanan tattara bayanai
Diamita Tsawon Nauyi
1.60 mm

2.40 mm

3.20 mm 1000 mm

1000 mm

1000 mm5 kg

5 kg

5 kg

 