Electrode mai ƙarancin hydrogen carbon ƙarfe E6011

Takaitaccen Bayani:

AWS E6011na'urar waldanau'in sinadarin cellulose potassium ne, wanda ake amfani da shi don walda a tsaye. Dukansu don walda AC da DC.


Cikakken Bayani game da Samfurin

Alamun Samfura

Aikace-aikace
Sandunan walda AWS E6011 ya dace da tsarin tasoshin walda kamar gine-gine da gadoji, tankunan ajiya, bututu da kayan haɗin matsi.

AWS E6011na'urar waldaNau'in sinadarin cellulose potassium ne, wanda ake amfani da shi don walda a tsaye. Dukansu don walda AC da DC. Yana ɗaukar fasahar waje mai ci gaba kuma yana da kyawawan halayen fasaha na walda. Ya kamata a sarrafa tsawon ARC a cikin iyaka mai dacewa. Ba walda mai laushi da murfin da ya dace ba ne.

Sinadaran da ke cikinsa (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Kayayyakin Inji na Karfe da aka Ajiye
Kayan Gwaji Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Darajar Garanti ≥420 ≥330 ≥22 ≥47
Sakamako na Gabaɗaya 485 380 24 86
Na'urar Haɓakawa (DC)
diamita φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Amperage 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

IRIN HALITTA: Direct Current Electrode Positive (DCEP) ko AC

DABARUKAN WALDA DA AKA SHAWARA:

Tsawon Baka - Matsakaicin tsayi (1/8" zuwa 1/4")

Faɗi - Ka kasance a gaban kududdufi kuma ka yi amfani da ɗan motsi na bulala

Kwance - Elektrode mai kusurwa kaɗan zuwa saman farantin

Tsaye a Sama - Ƙaramin bulala ko dabarar saƙa

Tsaye Ƙasa - Yi amfani da ƙarfin amperage mai girma da tafiya cikin sauri, kasancewa a gaba da kududdufi

Sama - Ka kasance a gaban kududdufi kuma ka yi amfani da ɗan motsi na bulala

Hankali:
1. Yana da sauƙin fallasa ga danshi, don Allah a ajiye shi a cikin yanayin bushewa.
2. Yana buƙatar dumamawa lokacin da fakitin ya karye ko kuma danshi ya sha, zafin dumama ya kamata ya kasance tsakanin 70C zuwa 80C, lokacin dumama ya kamata ya kasance daga awa 0.5 zuwa 1.
3. Lokacin amfani da na'urorin walda masu ƙarfin 5.0mm, ya fi kyau a yi amfani da ƙarfin lantarki mai ƙarfi, mai ƙarancin wutar lantarki, domin inganta aikin walda.