E6010 na'urar walda ta carbon steel

Takaitaccen Bayani:

E6010 wani nau'in lantarki ne na rutile-cellulosic sodium.


Cikakken Bayani game da Samfurin

Alamun Samfura

AWS E6010 Mai Sauƙin Walda na Karfe

AIKACE-AIKACE:

Ya dace da walda tsarin ƙarfe mai ƙarancin carbon kamar bututun mai, gina jiragen ruwa da gada da sauransu.

RANGWAME:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

HALAYEN NAN:

E6010 wani nau'in lantarki ne na sodium mai rutile-cellulosic. Ana iya walda shi don duk matsayi (musamman ga matsayi a tsaye-ƙasa) tare da DC+ kawai. Yana da kyakkyawan aikin walda kamar baka mai karko, ƙaramin fashewa, sauƙin cire slag da ikon sake dawowa da sauransu. Ingantaccen sarrafa wurin wanka mai narkewa, ƙarfin baka mai ƙarfi da zurfin shiga cikin ruwa a tsaye-ƙasa.

SIMINI NA DUKKAN KARFEN WALDA: (WT. %)

Abubuwa C Mn Si S P Ni Cr Mo V
Bukatu ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Sakamakon da Aka Saba 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

ABUBUWAN INJI NA DUKKAN KARFEN WALDA:

Abubuwa Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Bukatu ≥430 ≥330 ≥20 ≥27
Sakamakon da Aka Saba 475 400 26 80

HANKALI:

1. Gabaɗaya, ba sai an sake busar da wutar lantarki kafin walda ba. Idan danshi ya shafe shi, ya kamata a sake busar da shi a zafin 70℃-90℃ na tsawon awa 1.

2. Dole ne a cire tsatsa, mai, ruwa da sauran ƙazanta na yankin walda kafin a yi walda.

YADDA AKE YIN AIKI NA AL'ADA: ( DC+)

Diamita (mm) 2.5 3.2 4.0 5.0
Tsawon (mm) 300 350 400 400
Na yanzu (A) 50-80 60-100 100-140 140-180

MAKUNSHIN:

5kg/akwati, akwati 4/kwali, kilogiram 20/kwali, kwali 50/pallet. 21MT -26MT ga kowace 1X20″ FCL.

 

OEM/ODM:

Muna tallafawa OEM/ODM kuma muna iya yin marufi bisa ga ƙirar ku, da fatan za a tuntuɓe mu don tattaunawa dalla-dalla.

 

Halaye akan Amfani:

Bakin da ya tsaya cak sosai.

Kyakkyawan cire slag.

Shiga ciki ba shi da zurfi.

Kyakkyawan juriya ga zafi da tsatsa.

Kyakkyawan juriya ga tsagewa.


  • Na baya: