Low Alloy Karfe Welding Electrode AWS E7018-G Sandunan Welding Ƙarfe da Ƙarfin Hydrogen

Takaitaccen Bayani:

J507FeNi (AWS E7018-G) ƙaramin allo ne na ƙarfe na ƙarfe tare da foda baƙin ƙarfe da ƙaramin murfin hydrogen.Ana iya amfani da shi don duk-wuri waldi tare da AC da DC


Cikakken Bayani

Tags samfurin

Low Alloy Karfe Welding Electrode

J507FeNi                                                    

GB/T E5018-G

AWS E7018-G

Bayani: J507FeNi ƙaramin alloy karfe electrode tare da foda baƙin ƙarfe da ƙaramin murfin hydrogen.Ana iya amfani da shi don duk-wuri waldi tare da AC da DC.Tsawon aikin walda AC ya yi ƙasa da na waldi na DC

Aikace-aikacen: Ana amfani da shi don walƙiya matsakaicin ƙarfe na ƙarfe da tasoshin ƙarfin ƙarfe mai ƙarancin zafin jiki, kamar 16MnDR, da sauransu.

Abubuwan sinadaran na weld karfe(%):

C

Mn

Si

Ni

S

P

≤0.08

0.80 ~ 1.30

≤0.65

1.20 ~ 2.00

≤0.030

≤0.030

 

Abubuwan kayan aikin walda:

Gwaji abu

 

Ƙarfin ƙarfi

Mpa

 

Ƙarfin bayarwa

Mpa

 

Tsawaitawa

%

 

Ƙimar tasiri (J)

-40 ℃

Garanti

≥490

≥390

≥22

≥54

 

Yadawa hydrogen abun ciki na ajiyar karfe: ≤6.0ml/100g (hanyar glycerin)

Duban X-ray: I grade

 

Shawarwari na yanzu:

Diamita na sanda
(mm) da

3.2

4.0

5.0

Welding Current

(A)

90 ~ 120

140 ~ 180

170 ~ 210

 

Sanarwa:

1. A lantarki dole ne a gasa ga 1 hour a game da 350 ℃ kafin walda aiki;

2. Yana da mahimmanci don tsaftace tsatsa, sikelin mai, ruwa, da ƙazanta akan sassan walda kafin walda.

 

Wenzhou Tianyu Electronic Co., Ltd. da aka kafa a 2000. Mun aka tsunduma a cikin masana'antu nawalda lantarkis, sandunan walda, da kuma abubuwan amfani da walda fiye da shekaru 20.

Babban samfuranmu sun haɗa da bakin karfewalda lantarkis, carbon karfe waldi lantarki,low gami waldi lantarki, Surfacing waldi electrodes, nickel & cobalt gami waldi lantarki, m karfe & low gami waldi wayoyi, bakin karfe walda wayoyi, gas-garkuwar juyi cored wayoyi, aluminum walda wayoyi, submerged baka waldi.wayoyi, nickel & cobalt alloy walda wayoyi, tagulla walda wayoyi, TIG & MIG walda wayoyi, tungsten electrodes, carbon gouging lantarki, da sauran walda na'urorin & consumables.

 