Wayar Walda ta Nickel Alloy ERNiFeCr-1, Wayar Cika Wayar Nickel Tig Karfe

Takaitaccen Bayani:

Alloy 825 (ERNiFeCr-1) waya ce ta nickel-iron-chromium wadda ta sa wannan ya zama zaɓi mai dacewa don aikace-aikace iri-iri masu wahala.


Cikakken Bayani game da Samfurin

Alamun Samfura

Alloy na NickelWayar WaldaWayar TigERNiFeCr-1

Ma'auni
TS EN ISO 18274 - Ni 8065 - NiFe30Cr21Mo3
AWS A5.14 – ER NiFeCr-1

 

Fasaloli da Aikace-aikace

Alloy 825 shinenickelwaya mai ƙarfe-chromium wanda hakan ya sa wannan ya zama zaɓi mai dacewa don aikace-aikace iri-iri masu wahala.

Wannan waya tana ba da babban matakin juriya ga tsatsa ga muhalli mai narkewar iskar oxygen da kuma rage iskar oxygen.

Ya dace da rufin da aka rufe inda ake buƙatar irin wannan sinadari.

Kyakkyawan walda tare da cikakken ƙarfin walda mai austenitic tare da juriya mai ƙarfi ga tsatsagewar damuwa a cikin kafofin watsa labarai waɗanda ke ɗauke da ions na chloride.

Yawanci ana amfani da shi a masana'antun sarrafa sinadarai, man fetur, kera takarda da samar da wutar lantarki da sauransu.

 

Kayan Tushe na Al'ada

G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, GLOY 825, N08028, UNS N08825 W.Nr: 1.4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465, 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* Jerin misalai, ba cikakken bayani ba

 

Sinadarin Sinadarai %

C%

Mn%

Fe%

P%

S%

Si%

 

matsakaicin

0.70

22.00

matsakaicin

matsakaicin

matsakaicin

 

0.05

0.90

minti

0.020

0.004

0.50

 

 

Ku%

Ni%

Al%

Ti%

Cr%

Mo%

 

2.30

43.00

matsakaicin

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

Kayayyakin Inji
Ƙarfin Taurin Kai ≥550 MPa  
Ƙarfin Ba da Kyauta -  
Ƙarawa -  
Ƙarfin Tasiri -  

Kayayyakin injiniya suna da ƙima kuma suna iya bambanta dangane da zafi, iskar gas mai karewa, sigogin walda da sauran abubuwa.

 

Iskar Gas Mai Kariya

TS EN ISO 14175 TIG: I1 (Argon)

 

Wurare na Walda

TS EN ISO 6947 - PA, PB, PC, PD, PE, PF, PG

 

Bayanan Marufi
diamita Tsawon Nauyi  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 

Alhaki: Duk da cewa an yi duk mai yiwuwa don tabbatar da daidaiton bayanin da ke ciki, wannan bayanin yana iya canzawa ba tare da sanarwa ba kuma ana iya ɗaukarsa a matsayin wanda ya dace da jagora na gaba ɗaya.

 