AWS ERNiCrMo-7 Nickel Alloy Welding Wire Mig da Tig Wire, Arc Welding Rods Mafi kyawun mai samar da walda

Takaitaccen Bayani:

Ana amfani da ERNiCrMo-10 don waldawa kayan tushe na nickel-chromium-molybdenum ga kansu, ƙarfe da sauran abubuwan haɗin ginin nickel, da kuma kayan kwalliyar ƙarfe.Ana iya amfani dashi don walda duplex, super duplex bakin karfe.


Cikakken Bayani

Tags samfurin

BAYANIN KYAUTATA:

Saukewa: A5.14

Yayi daidai da Takaddun shaida: AWS A5.14 ASME SFA A5.14

Tsarin walda: GMAW & ASAW Tsarin walda

Ana amfani da ERNiCrMo-10 don waldawa kayan tushe na nickel-chromium-molybdenum ga kansu, ƙarfe da sauran abubuwan haɗin ginin nickel, da kuma kayan kwalliyar ƙarfe.Ana iya amfani dashi don walda duplex, super duplex bakin karfe.

Abubuwan Bukatun Haɗin Kemikal AWS

C = 0.015 max Ku = 0.50 max
Mn = 1.0 max Ni = Rago
Fe = 3.0 max Co = 2.0 max
P = 0.04 max Cr = 14.0 - 18.0
S = 0.03 max Mo = 14.0 - 18.0
Si = 0.08 max W = 0.50 max
Sauran = 0.50 max Ti = 0.70 max

Da fatan za a KIIRA DOMIN KARIN BAYANI DA MANYAN KYAUTA:

Aikace-aikace

Ana amfani da ERNiCrMo-7 don walda kayan tushe na nickel-chromium-molybdenum zuwa kanta, ƙarfe da sauran abubuwan haɗin nickel kuma don cladding karfe tare da kayan weld na NI-CR-MO

KYAUTA KYAUTA:

Haɗin Kemikal % (Na yau da kullun)
C = 0.01 Cr = 16.5 Ni = Balance
Fe = 2.20 Mo = 15.75
An Ajiye Duk Kayayyakin Karfe na Weld% (AW)
Ƙarfin Ƙarfin Ƙarfi 113,00 psi
Tsawaitawa 29%

ABINDA AKE YIWA KYAUTA KYAUTA CHRPY-V-NOCH:

Bai dace ba

Shawarar Ma'aunin Welding don MIG da SAW Welding na Nickel Alloys
Tsari Diamita na Waya Voltage (V) Amperage (A) Gas
MIG .035 inci 26-29 150-190 75% Argon + 25% Helium
.045 inci 28-32 180-220 75% Argon + 25% Helium
1/16 inci 29-33 200-250 75% Argon + 25% Helium
SAW 3/32 inci 28-30 270-350 Za a iya amfani da madaidaicin Flux.
1/8 inci 29-32 350-450 Za a iya amfani da madaidaicin Flux.
5/32 inci 30-33 400-550 Za a iya amfani da madaidaicin Flux.