Alloy na NickelWayar Walda Wayar TigENiFe-CI
| Ma'auni |
| EN ISO 1071 – SC NiFe-1 |
| AWS A5.15 - E NiFe-CI |
Fasaloli da Aikace-aikace
Ferro-nickelwaya mai ƙarfi da ake amfani da ita don walda ƙarfe mai siminti da ƙarfe mai ductile.
Ya dace da haɗin gwiwa daban-daban tsakanin ƙarfe mai siminti, ƙarfe mai laushi, ƙarancin ƙarfe da ƙarfe mai bakin ƙarfe.
Ana ba da shawarar yin walda mai yawan sulfur, phosphorus ko simintin da ya gurɓata da man shafawa.
Ana amfani da shi galibi don aikace-aikacen gyara da ƙera abubuwa daban-daban, gami da sake gina shafts, ƙafafun, haɗin gwiwa masu mahimmanci tsakanin ƙarfe da ƙarfen siminti da sauransu.
Kayan Tushe na Al'ada
ƙarfe mai launin toka, mai laushi, mai ƙusa*
* Jerin misalai, ba cikakken bayani ba
| Sinadarin Sinadarai % | ||||||
| C% | Mn% | Si% | P% | S% | ||
| matsakaicin | matsakaicin | matsakaicin | matsakaicin | matsakaicin | ||
| 2.00 | 0.80 | 0.20 | 0.03 | 0.03 | ||
|
|
|
|
|
| ||
| Fe% | Ni% | Ku% | Al% |
| ||
| sake. | 54.00 | matsakaicin | matsakaicin |
| ||
|
| 56.00 | 2.50 | 1.00 |
| ||
| Kayayyakin Inji | ||
| Ƙarfin Taurin Kai | 400 – 579 MPa | |
| Ƙarfin Ba da Kyauta | - | |
| Ƙarawa | - | |
| Ƙarfin Tasiri | - | |
Kayayyakin injiniya suna da ƙima kuma suna iya bambanta dangane da zafi, iskar gas mai karewa, sigogin walda da sauran abubuwa.
Iskar Gas Mai Kariya
TS EN ISO 14175 TIG: I1 (Argon)
Wurare na Walda
TS EN ISO 6947 - PA, PB, PC, PD, PE, PF
| Bayanan Marufi | |||
| diamita | Tsawon | Nauyi |
|
| 1.60 mm 2.40 mm 3.20 mm | 1000 mm 1000 mm 1000 mm | 5 Kg 5 Kg 5 Kg |
|
Alhaki: Duk da cewa an yi duk mai yiwuwa don tabbatar da daidaiton bayanin da ke ciki, wannan bayanin yana iya canzawa ba tare da sanarwa ba kuma ana iya ɗaukarsa a matsayin wanda ya dace da jagora na gaba ɗaya.