Kayan Walda na AWS E8016-G Masu Walda Masu Ƙarfin Alloy Karfe Masu Walda Masu Ƙarfi Kayan Walda na Stick Arc

Takaitaccen Bayani:

J556 (AWS E8016-G) wani lantarki ne mai ƙarancin ƙarfe mai kauri wanda ke da rufin sinadarin hydrogen potassium mai ƙarancin hydrogen. Ana iya amfani da AC da DC duka, kuma ana iya haɗa su a kowane matsayi.


Cikakken Bayani game da Samfurin

Alamun Samfura

Ƙaramin Walda na Karfe

J556

GB/T E5516-G

AWS E8016-G

Bayani: J556 wani lantarki ne mai ƙarancin ƙarfe mai rufi mai ƙarancin sinadarin hydrogen potassium. Ana iya amfani da AC da DC duka, kuma ana iya haɗa su a kowane matsayi. Daidaiton aikin walda na AC ya ɗan yi ƙasa da na walda kai tsaye.

Aikace-aikace: Ana amfani da shi don walda ƙarfe mai matsakaicin carbon da tsarin ƙarfe mai ƙarancin ƙarfe kamar Q390.

 

Sinadarin sinadarai na ƙarfen walda(%):

C

Mn

Si

S

P

≤0.12

≥1.00

0.30 ~ 0.70

≤0.035

≤0.035

 

Kayan aikin injiniya na ƙarfe na walda:

Gwaji abu

Ƙarfin tauri

Mpa

Ƙarfin bayarwa

Mpa

Ƙarawa

%

Ƙimar tasiri (J)

-30℃

An Garanti

≥540

≥440

≥17

≥27

An gwada

550 ~ 620

≥450

22 ~ 32

—

 

Yaɗuwar sinadarin hydrogen a cikin ƙarfe da aka ajiye: ≤6.0mL/100g (hanyar glycerin)

 

Duba X-ray: I maki

 

Shawarar da ake bayarwa:

Diamita na sanda

(mm)

2.5

3.2

4.0

5.0

Walda na yanzu

(A)

60 ~ 90

80 ~ 110

130 ~ 170

160 ~ 200

 

Sanarwa:

1. Dole ne a gasa wutar lantarki na tsawon awa 1 a zafin 350℃ kafin a fara aiki da walda;

2. Yana da mahimmanci a tsaftace tsatsa, ma'aunin mai, ruwa, da ƙazanta a kan sassan walda kafin walda;

3. Yi amfani da aikin gajeriyar baka lokacin walda. Hanyar walda mai kunkuntar ta dace;

4. Haɗa lantarki zuwa sandar da ke da kyau lokacin aiki akan DC.

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 