AWS A5.4 E310-16 Bakin Karfe Walda Kayan Walda Sanda

Takaitaccen Bayani:

A402 (AWS E310-16) wani electrode ne na bakin karfe mai tsabta na Cr26Ni21 mai rufin sinadarin calcium na titanium.


Cikakken Bayani game da Samfurin

Alamun Samfura

Bakin Karfe Walda Electrode

A402                                   

GB/T E310-16

AWS A5.4 E310-16

 Bayani: A402 wani electrode ne mai tsabta na Cr26Ni21 mai launin austenitic mai rufin calcium na titanium. Ana iya amfani da shi don AC da DC tare da kyakkyawan aikin aiki. Karfe da aka ajiye yana da kyakkyawan juriya ga iskar shaka a ƙarƙashin yanayin zafi mai zafi na 900 ~ 1100 ℃.

Aikace-aikace: Ana amfani da shi don walda irin wannan nau'in bakin ƙarfe mai jure zafi wanda ke aiki a ƙarƙashin yanayin zafi mai yawa, kuma ana iya amfani da shi don walda na ƙarfe chromium masu tauri (kamar Cr5Mo, Cr9Mo, Cr13 da Cr28, da sauransu) da ƙarfe daban-daban.

 

 

Sinadarin sinadarai na ƙarfen walda(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

0.08 ~ 0.20

1.0 ~ 2.5

≤0.75

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

≤0.75

≤0.030

≤0.030

 

 

Kayan aikin injiniya na ƙarfe na walda:

Gwaji abu

Ƙarfin tauri

Mpa

Ƙarawa

%

An Garanti

≥550

≥25

 

Shawarar da ake bayarwa:

Diamita na sanda

(mm)

2.0

2.5

3.2

4.0

5.0

Walda na Wuta

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

 

Sanarwa:

  1. Dole ne a gasa wutar lantarki na tsawon awa 1 a kusan 250℃ kafin aikin walda;
  2. Saboda zurfin shigar ciki ba shi da zurfi yayin walda ta AC, ya kamata a yi amfani da wutar lantarki ta DC gwargwadon iyawa don samun zurfin shigar ciki. Kuma kada wutar ta yi girma sosai don guje wa jajayen sandar walda.

 

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 

 

 


  • Na baya:
  • Na gaba: