AWS A5.4 E312-17 Bakin Karfe Welding Electrodes Arc Stick Welding Rods

Takaitaccen Bayani:

AWS E312-17 duk matsayi ne kuma yayi kama da 312-16 amma rufin -17 ya ƙunshi ƙarin silica da ƙasa da titani-um yana haifar da tasirin "Fsa-Arc" lokacin da aka yi amfani da shi akan waldawar fillet na kwance.


Cikakken Bayani

Tags samfurin

AWS E312-17 duk matsayi ne kuma yayi kama da 312-16 amma rufin -17 ya ƙunshi ƙarin silica da ƙasa da titani-um yana haifar da tasirin "Fsa-Arc" lokacin da aka yi amfani da shi akan waldawar fillet na kwance.

Rabewa:

AWS A5.4 E312-17

ISO 3581-A E29 9 R 1 2

BAYANI BAYANI

Babban rutile-mahimmancin babban CrNi-alloyed duk matsayin lantarki

Madalla don gyaran walƙiya

Musamman ƙera don karafa masu wahalar walda, kamar faranti sulke, austenitic Mn-karfe da manyan C-karfe.

Excellent weldability da kai sakewa slag

Weldable akan AC da DC+ polarity

Nau'in yanzu: DC/AC+

Abubuwan Sinadarai na Inweld 312-17

Fe

C

Cr

Ni

Mo

Mn

Si

P

S

N

Cu

Ma'auni

0.15

28.0

8.0

0.75

0.5-2.5

0.90

0.04

0.03

---

0.75

- 32.0

-10.5

Ƙimar guda ɗaya tana da iyaka sai dai in an kayyade.

Bayani da Aikace-aikace

AWS E312-17 duk matsayi ne kuma yayi kama da 312-16 amma rufin -17 ya ƙunshi ƙarin silica da ƙarancin titani-um yana haifar da tasirin "Fsa-Arc" lokacin amfani da walƙiyar fillet a kwance.Wannan kuma yana samar da ajiya mai walƙiya tare da mafi kyawun kyan gani wanda ya fi lebur don haɗawa.312-17 yana da saurin daskarewa daskarewa yana ba shi mafi kyawun halaye lokacin amfani da dabarar ja.Kyakkyawan zaɓi akan ƙarfe masu wahala-zuwa walda irin su ƙarfe mai ƙarfi na iska, matsakaici da babban ƙarfe na carbon.Cikakken na'urar lantarki da za a yi amfani da shi inda karfen tushe ba a sani ba na ƙarfe.Dace da yawa dissimilar aikace-aikace shafe manganese-hardening karfe, makamai karfe, spring karfe, dogo karfe, nickel clad karfe, kayan aiki & mutu karfe da jirgin sama karfe.Yawanci ana amfani da shi azaman gini mai jurewa lalacewa da Layer “buffer” a cikin aikace-aikacen fuskantar wuya.Aiki ya taurare har zuwa 200 Brinell.312-17 yana da mafi girman juzu'i da ƙarfin samar da daidaitattun na'urorin lantarki masu rufin bakin karfe (bakin duplex ba a haɗa shi ba).

Abubuwan da aka Shawarar

SMAW (DCEP - Electrode+)

Diamita Waya

Amperage

3/32”

50-80

1/8”

7-110

5/32”

100-140