Sandar da ke da ƙarfi ta Premium D132 (B-83) Tana Ba da Kariyar Fuskar da ke Dorewa

D132(B-83)Sandar da ke fuskantar ƙarfiYana tsaye a matsayin na'urar lantarki ta musamman mai ƙarancin hydrogen wanda aka ƙera don ayyukan walda masu mahimmanci. Wannan sandar walda ta baka ta yi fice wajen dawo da abubuwan da suka lalace waɗanda ke fuskantar matsin lamba mai matsakaici da kuma ƙarfin matsawa. An sanya ta a matsayin sandar walda ta saman da kuma mafita ta sake ginawa, tana samar da baka mai ƙarfi, mai ƙarancin splatter yayin da take rage haɗarin fashewa da hydrogen ke haifarwa. Tsarinta yana tabbatar da santsi da kuma kamannin beads masu daidaito, wanda hakan ya sa ya dace da gyaran injunan masana'antu, kayan aikin noma, da sassan motoci waɗanda ke buƙatar gyara girma da taurare saman.

 

Bayanan fasaha suna nuna sandar'Ƙarfin s na musamman. Ƙarfe mai ɗaukuwa yana nuna ƙarfin matsi mai yawa kuma yana kiyaye ingantaccen injin aiki–yana ba da damar ayyukan bayan walda kamar juyawa, niƙa, da kuma shimfiɗa ba tare da ɓatar da mutunci ba. Wannan halayyar tana da matuƙar amfani ga abubuwan da ke buƙatar jurewa mai ƙarfi bayan an gama su. An rarraba ta a matsayin ƙaramin lantarki mai ƙarancin hydrogen, yana rage yawan ramuka da saurin fashewa da sanyi sosai, musamman a cikin sassa masu kauri ko gidajen haɗin gwiwa masu ƙarfi. Tsarin kwararar da aka daidaita yana samar da rabuwar slag kuma yana rage yawan splatter, yana haɓaka ingancin aiki.

 

Ga aikace-aikacen da ke buƙatar juriya ga matsakaicin lalacewa,Sandar da ke fuskantar ƙarfiyana ba da kyakkyawan aiki. Haɗin ƙarfe yana ƙirƙirar wani yanki mai tauri, mai tauri wanda ke magance lalacewar da ke lalata abubuwa a cikin muhalli kamar sarrafa kayan da yawa, motsa ƙasa, ko ƙera su yadda ya kamata. Ba kamar madadin masu rauni ba, D132(B-83)'Tanadar s tana shan kuzarin tasiri yayin da take kiyaye taurin saman, tana ƙara tsawon rayuwar aikin sassan sosai. Ya dace musamman don sake gina shafts, birgima, sassan murƙushewa, da ruwan wukake na masana'antu waɗanda ke fuskantar gogayya da matsin lamba akai-akai.

 

Sakamakon da ya fi kyau yana buƙatar bin ƙa'idodin walda: A kunna abubuwan da ke ciki zuwa 250-300°C (482-572)°F) bisa ga nauyi, kula da yanayin zafi na interpass, da kuma amfani da DC reverse polarity (electrode positive). Ajiye sandunan a cikin kwantena da aka rufe a 250-300.°F (121-149)°C) sannan a sake gasawa idan an fallasa shi ga danshi fiye da kashi 50% na tsawon sama da awanni 4. A ajiye beads a cikin kunkuntar matsewa don sarrafa narkewar da kuma ƙara tauri. Ana ba da shawarar a yi amfani da shi a hankali a ƙarƙashin rufin bayan an yi walda don amfani mai mahimmanci don hana gurɓatar hydrogen.

 

D132(B-83)Sandar da ke fuskantar ƙarfiyana ba da mafita mai inganci, mai inganci don yaƙi da lalacewa da dawo da girma. Ƙarfinsa mai ƙarancin hydrogen, tare da ƙarfin matsewa da juriyar lalacewa mai sarrafawa, ya sa wannan sandar walda ta saman ta zama dole don gyarawa da sake gina shirye-shiryen a cikin manyan masana'antu. Ta hanyar zaɓar wannan lantarki, injiniyoyi suna tabbatar da cewa kayan da aka gyara sun dawo da aikin asali yayin da suke cimma tsawon rai na aiki a ƙarƙashin yanayi mai wahala.

Sandar da ke fuskantar ƙarfi