H10MnSi AWS EM13K Ruwan Welding Arc Mai Ruwa

Takaitaccen Bayani:

H10MnSi Submerged baka waldi waya nau'i ne na matsakaici-manganese da matsakaici-silicon irin walda waya.


Cikakken Bayani

Tags samfurin

H10MnSi AWS EM13K Ruwan Welding Arc Mai Ruwa

EM13K 2.5/3.2/4.0/5.0mm Waya Welding Arc

H10MnSi Submerged baka waldi waya nau'i ne na matsakaici-manganese da matsakaici-silicon irin walda waya.
1. Yana daidaita da matsakaici-manganese da matsakaici-siliki irin walda juzu'in.
2. Ba shi da kula da tsatsa akan karfen tushe.
3. Yana da kyau kwarai dutse gyare-gyare da slag detachability.
4. Monopole ko dipole.AC/DC.
5. Ana amfani da duka biyu high gudun waldi da kuma cika waldi a kan 50kg class tushe karafa.
6. waldi na sauran 501 Mpa matakin carbon karfe da ƙananan gami karfe

EM13K Daidaita zuwa Matsayi: GB/T 5293 H10MnSi
Saukewa: EM13K
ISO 14171-B-SU25

Ƙayyadaddun bayanai: Yana da nau'in walda mai nau'i mai dacewa tare da manganese da abun ciki na siliki mai dacewa., Ya dace da ƙananan manganese da ƙananan nau'in siliki na walƙiya, Rashin hankali ga tsatsa a kan tushe karfe.Yana da kyakkyawan gyare-gyaren ƙwanƙwasa, kyakkyawan ikon cire shinge.

Manufa: Yin amfani da sintered juzu'i LT.SJ101, ana iya amfani da shi duka biyu don high-gudun waldi karfe farantin karfe na tensile ƙarfi 420N/mm2 da ciko waldi.An yadu amfani da walda tukunyar jirgi, matsa lamba jirgin ruwa, gada, jirgi da dai sauransu.

Haɗin Sinadari(%)

 

 

Haɗin Sinadari C Mn Si S P Cr Ni Cu
Garanti Darajar ≤0.14 0.80 ~
1.10
0.60 ~
0.90
≤0.035 ≤0.035 ≤0.20 ≤0.30 ≤0.35
Sakamakon Gabaɗaya 0.089 0.98 0.67 0.023 0.032 0.015 0.034 0.11

 
Kayayyakin Injini na Ƙarfe Mai Adadi

Gwaji abu

Flux

Rm (MPa) ReL/Rp0.2(MPa) A(%) KV2(J)
-20 ℃
LT•SJ101 415-550 ≥330 ≥22 ≥27

 
Girman Wayoyin walda

Girman (mm) Φ2.5 Φ3.2 Φ4.0 Φ5.0

 