Wayar Flux-Cored EC410NiMo

Takaitaccen Bayani:

EC410NiMo waya ce mai kama da bakin karfe mai kama da martensitic wadda aka yi da flux core wadda ke ɗauke da sinadarai masu ɗauke da 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, da kuma 0.40 – 0.70% Mo.

Cikakken Bayani game da Samfurin

Alamun Samfura

Daidaitaccen Daidaito

GB/T 17853-2018 TS410NiMo-FC11

AWS A5.22M-2012 E410NiMoT1-1

Daidaitaccen abu: 13Cr-4Ni (EN1.4313/UNS S41500)

Bayani

EC410NiMo waya ce mai kama da bakin karfe mai kama da martensitic wadda aka yi da flux core wadda ke ɗauke da sinadarai masu ɗauke da 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, da kuma 0.40 – 0.70% Mo. Ya dace da dukkan matsayi.walda mai siffar flux-core(FCAW) mai karko, ƙarancin fashewa, da kuma kyakkyawan cirewar slag. Karfe da aka ajiye yana da kyakkyawan juriyar lalacewa, juriyar fashewa, da kuma halayen injiniya. Ana ba da shawarar a yi zafi a 150 - 260℃, kuma a yi maganin zafi bayan walda (PWHT) a 590 ~ 620℃ na tsawon awa 1 (sannan a sanyaya iska, AC) bayan walda.

Aikace-aikace

Ya dace da walda ASTM CA6NM ƙarfe da ƙarfe mai lamba 13%Cr – 4%Ni. Ana amfani da shi don gyara layukan crane masu ƙarfi, na'urorin bugawa, sandunan ƙarfe, abubuwan da ke cikin wutar lantarki da aka sawa ta hanyar cavitation, da sassan tsarin da ke buƙatar juriya ga tsatsa da lalacewa.

Sinadarin Sinadarin Walda (%)

Sinadarin C Cr Ni Mo Mn Si P S Cu
Bukatar ≤0.06 11.0-12.5 4.0-5.0 0.40-0.70 ≤1.00 ≤1.00 ≤0.040 ≤0.030 ≤0.75
Sakamakon Gwaji 0.02 12.3 4.65 0.54 0.59 0.33 0.023 0.01 0.01

Kayayyakin Inji na Karfe da aka Ajiye

Sunan Gwaji Ƙarfin Tashin Hankali (MPa) Ƙarawa% X-Ray Gwajin Tasiri(+20℃)J Taurin HB Ruwan Hydrogen Mai Yaɗuwa (ml/100g)
Bukatar ≥760 ≥15 Darasi na I – – ≤5
Sakamakon Gwaji 845 19 Darasi na I 60-90 250-310 ≤5

 

Shawarar Sigar Walda

Tushen Wutar Lantarki: DC Reverse (DC-)

Diamita da Waya:

Shawarar Yanzu:

Diamita na Sanda (mm) 3.2 4.0 5.0
Wutar Walda (A) 80-120 120-160 150-190

Sanarwa

1. A gasa wutar lantarki a 300℃ na tsawon awa daya kafin a yi amfani da ita don cire danshi.

2. Tsaftace tsatsa, mai, da danshi daga saman ƙarfe na tushe; yi amfani da aikin gajeriyar hanyar baka don ƙananan ƙusoshin walda.

3. Ya kamata a yi PWHT nan da nan bayan walda don guje wa lalacewa.

 

 