Tig da Mig Wire A5.28 ER80S-D2, Ƙarfe Mai Rarraba Ƙarfe don Welding Arc Garkuwar Gas

Takaitaccen Bayani:

ER80S-D2 waya ce mai laushi ta ƙarfe da ake amfani da ita a cikin yanayi inda porosity ke da matsala ko lokacin da dole ne ka magance babban sulfur ko abun cikin carbon a cikin ƙarfen ka.


Cikakken Bayani

Tags samfurin

A5.28 ER80S-D2, Ƙarfe-Ƙaramar Filler Karfe don Welding Arc Garkuwar Gas

ER80S-D2 waya ce mai laushi ta ƙarfe da ake amfani da ita a cikin yanayi inda porosity ke da matsala ko lokacin da dole ne ka magance babban sulfur ko abun cikin carbon a cikin ƙarfen ka.Ya ƙunshi manyan matakan manganese da silicon don samar da jika mai kyau da kuma tsatsa mai kyau da juriya.

Yawanci Aikace-aikace: x-ray ingancin aikace-aikace, high-ƙarfi welds, tururi tukunyar jirgi, matsa lamba tankuna, gas bututu, zafi musayar, petrochemical masana'antu.

Saukewa: ER80S-D2 Takaddun shaida: AWS A5.28/A5.28M:2005
Saukewa: ER80S-D2 AWS/ASME SFA A5.28

 

Matsayin walda: F, V, OH, H Yanzu:
GMAW-DCEP

 

Ƙarfin Ƙarfin Ƙarfi, kpsi: 80 min
Ƙarfin Haɓaka, kpsi: 68 min
Tsawaita %: 17 min

Chemistry na Waya na yau da kullun kamar na AWS A5.28 (ƙimomi guda ɗaya ne mafi girman)

C Mn Si P S Ni Mo Cu Sauran
0.07-0.12 1.60-2.10 0.50-0.80 0.025 0.025 0.15 0.40-0.60 0.50 0.50
Ma'aunin walda na al'ada
Diamita Tsari Volt Amps Garkuwar Gas
in (mm)
.035 (0.9) GMAW 28-32 165-200 Fesa canja wurin 98% Argon / 2% Oxygen
.045 (1.2) GMAW 30-34 180-220 Fesa canja wurin 98% Argon / 2% Oxygen
1/16 (1.6) GMAW 30-34 230-260 Fesa canja wurin 98% Argon / 2% Oxygen
.035 (0.9) GMAW 22-25 100-140 Canja wurin gajeriyar kewayawa 90% Helium / 75% Argon / 25% CO2
.045 (1.2) GMAW 23-26 120-150 Canja wurin gajeriyar kewayawa 90% Helium / 75% Argon / 25% CO2
1/16 (1.6) GMAW 23-26 160-200 Canja wurin gajeriyar kewayawa 90% Helium / 75% Argon / 25% CO2
1/16 (1.6) GTAW 12-15 100-125 100% Argon
3/32 (2.4) GTAW 15-20 125-175 100% Argon
1/8 (3.2) GTAW 15-20 175-250 100% Argon

 


  • Na baya: