ER330 Bakin Karfe Welding Wire MIG da TIG Welding Rods Filler Sanduna

Takaitaccen Bayani:

Bakin karfe waldi waya yana da high cladding yadda ya dace, mai kyau waldi fasaha yi a duk-wuri waldi.Ana amfani da su sosai a masana'antu: tsarin gine-gine, abin hawa, injiniyan gada, injin ma'adinai, titin jirgin ƙasa, bututun mai, kayan aiki mai ɗaukar iskar gas, kayan wuta, da sauransu.


Cikakken Bayani

Tags samfurin

Rarraba AWS: AWS 5.9

BAYANI:

Bakin karfe waldi waya yana da high cladding yadda ya dace, mai kyau waldi fasaha yi a duk-wuri waldi.Ana amfani da su sosai a cikin masana'antu: tsarin gini, abin hawa, injiniyan gada, injin ma'adinai, titin jirgin ƙasa, bututun mai, kayan aiki mai ɗaukar iskar gas, kayan wuta, da sauransu.

MISALI NO.& GIRMAN:

1. Factory wadata sabis na OEM.

2. Model: ER308 ER308L ER308Lsi ER309 ER309L ER316 ER316L ER316Lsi da dai sauransu.

3. Girman waya MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4.TIG girman waya: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.

GABATARWA:

Muna samar da nau'ikan waya daban-daban na bakin karfe, gami da Mig m waya waldawa, Tig rod waya da igiyar walda mai nutsewa-baka, duk masu inganci kuma ana siyar dasu a duk duniya.

Ban da 308 da 309, muna kuma bayar da 304, 321, 347, 316L, 310, 2209, da 201. Haka kuma ƙayyadaddun bayanai na musamman kamar 318L, 904L, 2594, NiCrMo-3, Ni1.

CIKI:

Mig waldi packing (spool da drum pack)

Diamita: 0.8-2.0mm

Kunshin: 1 kg / spool, 5 kg / spool, 15 kg / spool, 20 kg / spool, 100 kg / drum, 200 kg / drum

Tig sanda waldi waya shiryarwa (roba tube)

Diamita: 1.0 - 5.0mm

Kunshin: 5 kg / fakiti

Submerted baka walda waya

Diamita: 2.5-5.0mm

Kunshin: 20kg/fakiti, 25kg/fakitin

Marufi na tsaka tsaki da OEM ana maraba!

RUWAN CUTAR KARFE WAYAR welding KARFE:

Model No.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304l

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

Saukewa: ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

Saukewa: ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

Saukewa: ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

Saukewa: ER308LSI

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

Saukewa: ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

Saukewa: ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

Saukewa: ER309LSI

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

Saukewa: ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

Saukewa: ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

Saukewa: ER316LSI

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

Saukewa: ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

Saukewa: ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

Saukewa: ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

Saukewa: ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

ABINDA AKE NUFI NA welding WIRE:

Model No.

Ƙarfin Tensile Rm (Mpa)

Ƙarfin Haɓaka Rel ko Rp0.2(Mpa)

Tsawaitawa

(%)

Model No.

Ƙarfin Tensile Rm (Mpa)

Ƙarfin Haɓaka Rel ko Rp0.2(Mpa)

Tsawaitawa

(%)

304

550

--

25

Saukewa: ER309LSI

510

320

25

304l

510

--

25

Saukewa: ER316

510

320

25

Saukewa: ER307

590

350

25

Saukewa: ER316L

510

320

25

Saukewa: ER308

550

350

25

Saukewa: ER316LSI

510

320

20

Saukewa: ER308L

510

320

25

Saukewa: ER310

550

350

25

Saukewa: ER308LSI

510

320

25

Saukewa: ER347

550

350

25

Saukewa: ER309

550

350

25

Saukewa: ER317

550

350

25

Saukewa: ER309L

510

320

25

Saukewa: ER321

550

350

25

TIG da MIG bakin karfe walda waya abun da ke ciki

YB5092-2005

AWS

Haɗin Sinadari%

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307S

0.075

0.78

6.7

0.022

0.01

19.8

8.8

Hoton H06Cr21Ni10

Saukewa: ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

Hoton H0OCr21Ni10

Saukewa: ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

Saukewa: H06Cr21Ni10S

ER308S

0.045

0.85

1.5

0.022

0.01

20.8

9.8

Hoton H06Cr24Ni13

Saukewa: ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

Hoton H03Cr24Ni13

Saukewa: ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

Saukewa: ER309LSI

0.018

0.8

1.7

0.02

0.01

23.5

13.5

Hoton H21Cr16Ni35

Saukewa: ER330

0.2

0.38

1.5

0.022

0.01

16.5

34.5

Saukewa: H06Cr19Ni12Mo2

Saukewa: ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

Saukewa: H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

Saukewa: H03Cr19Ni12Mo2

Saukewa: ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

Saukewa: H03Cr19Ni12Mo2Si

Saukewa: ER316LSI

0.06

0.85

1.7

0.022

0.01

18.8

12.6

2.4

Saukewa: H03Cr17Ni14Mo3

Saukewa: ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

Saukewa: ER318

0.06

0.42

1.5

0.022

0.01

18.5

11.8

2.3

Saukewa: H07Cr20Ni34Mo2Cu3Nb

Saukewa: ER320

0.06

0.4

1

0.022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

Saukewa: ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

Saukewa: ER321

0.06

0.45

1.5

0.022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

Saukewa: ER347

0.055

0.48

1.8

0.021

0.008

20.8

9.8

Nb1xC-1.0

Hoton H12Cr26Ni21

Saukewa: ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

Saukewa: H02Cr20Ni25Mo4Cu

Saukewa: ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

ku 1.80

Saukewa: H03Cr22Ni9Mo3N

Saukewa: ER2209

0.022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

Saukewa: H04Cr25Ni5Mo3Cu2N

Saukewa: ER2553

0.027

0.5

1

0.025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

Saukewa: ER312

0.09

0.38

1.5

0.022

0.01

29.5

8.5

Saukewa: H03Cr24Ni13MoL

ER309L Mo

0.023

0.45

1.5

0.022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

Saukewa: ER630

0.04

0.39

0.5

0.022

0.01

16.5

4.8

Ku;3 Nb;0.28

Hoton H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0.022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0.022

0.01

20.8

9.8

Saukewa: H05Cr22Ni11Mn6Mo3VN

Saukewa: ER209

0.04

0.4

4.5

0.022

0.01

21.5

10.8

2.2

N; 0.20 V; 0.18