ENiCrFe-3 Electrodes don Nickel

Takaitaccen Bayani:

Electrode yana cire ƙarfe mai ƙarfin 65Ni-20Cr-2Nb-1.5Mo.


Cikakken Bayani game da Samfurin

Alamun Samfura

Lambar ISO ta EN: 14172: ENi6082

Electrode yana ajiye ƙarfe mai nauyin 65Ni-20Cr-2Nb-1.5Mo. Ƙarfe mai ƙarfin rediyo mai inganci mai kyau. Ya fi dacewa da walda gami masu kama da juna, don walda tare da ƙarfe mai ƙarfe mai nauyin Nickel-Chromium lokacin da babban abun ciki na Manganese ba shi da illa, don walda gefen walda na ƙarfe mai nauyin Nickel Chromium-Iron da haɗin ƙarfe daban-daban. Ya dace da lulluɓe faranti na manne. An ba da shawarar musamman don walda ƙarfe 9% Ni don sabis na cryogenic. Hakanan ana amfani da shi don walda gami na Nickel-Chromium da ake amfani da su don aikace-aikacen zafi mai yawa kamar abubuwan dumama tanderu da bututun gyara.

ABUBUWAN DA KE CIKI NA KE CIKAKKEN SINADARI NA DUKKAN KARFE NA WALDA

Sinadarin C Mn Si Cr Ni Fe Nb Cu Ti S P
Kashi ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

ABUBUWAN DA AKA YI A KAN MAKARANTAR DUKKAN KARFEN WALDA

UTS YS Ƙarawa Ƙarfin Tasirin CVN (J) Faɗaɗawa ta gefe Ƙarfin Ragewa a
(MPa) (MPa) (L= 5d)% a Ƙananan 196°C a ƙasa da 196°C (mm) 600°C na tsawon awanni 1000.
620 500 30 75 0.85 160 MPa

BAYANAI NA GARGAJIYA DA RUFEWA: DC (+)

Girman (mm)

Dia x Tsawon

5×350

4×350

3.15 × 350

2.5×350

Nisan Yanzu (Amps)

150-180

120-150

80-110

60-70

Nauyi/Kwali (kg)

2.5

2.5

2.5

2.5

Gargaɗi

1. Tabbatar da cewa wayoyin lantarki sun bushe. Sake busar da wayoyin lantarki a zafin 300-325°C na tsawon awa daya.

2. A kiyaye gajeriyar baka, mai kauri sannan a rage zafin da ake fitarwa.

3. Bari walda ta huce zuwa ƙasa da digiri 50 na Celsius kafin ta yi sanyi, sai kuma ta yi ta gaba.