A5.13 ECoCr-C Cobalt Alloy Hardfacing Sandunan Welding Wear-resistant Welding Electrode Arc Welding Stick

Takaitaccen Bayani:

A5.13 ECoCr-C Cobalt Alloy Hardfacing Welding Rods ana amfani da waldi shugabannin bawul, hatimi zobba na high matsa lamba famfo da sassa na crushers.


Cikakken Bayani

Tags samfurin

 

Bayanin AWS:AWS A5.13/AME A5.13 ECoCr-C
APPLICATIONS:

Hard surfacing na bawul shugabannin, hatimi zobba na babban matsa lamba famfo da kuma sassan crushers.
BAYANI:

COBALTHARD 1FC na'urar da aka rufe shine mafi girman ma'auni mai ƙarfi a cikin rukunin cobalt gami da aka yi amfani da shi don haɓakar lalatawar zafin jiki mai alaƙa da lalata.Abubuwan ajiya na wannan gami suna da babban adadin chromium carbides waɗanda ke yin tasiri ga juriyar lalacewa.Bugu da kari na tungsten kara habaka high zafin jiki taurin da matrix taurin ga kyau kwarai m da kuma m barbashi yashwa lalacewa juriya.Yana haɗi da kyau tare da duk karafa, ciki har da bakin karfe.
BAYANI AKAN AMFANI:

Preheat a 300ºC kuma sama gaba ɗaya.Yi amfani da zafin jiki na PHILARC da ke nuna sanduna ko ma'aunin zafin jiki na PHILARC don tantance idan an cimma madaidaicin zafin jiki kafin walda.Don ƙarin cikakkun bayanai duba PHILARC Chart 4 Sauƙaƙan Matakai don walda.

Yana da tasiri don yin zafi a 600ºC kuma don rage sanyi bayan walda don hana fashewa.

Busasshen lantarki a 150-200ºC na minti 30 - 60 kafin amfani.Yi amfani da tanda mai bushewa PHILARC.

HARDNESS OF WELD METAL DEPOSIT: 50 - 56 HRC (520- 620 Hv)
HAKIKA CUTAR KARFE NA WELD (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Bal

MANYAN KYAUTA DA SHAWARAR YANZU ( DC +):

Girman (dia. mm) 3.2 4.0 5.0
Tsawon (mm) 350 350 350
Range na Yanzu (Amp) 90-120 110-150 140-180

 

 