AWS/ASME A 5.3 E4043 Aluminum Welding Electrodes

Takaitaccen Bayani:

L109 (AWS/ASME A 5.3 E 4043) wani tsararren lantarki ne na aluminum mai rufi mai tushen gishiri. Yi amfani da DCEP (mai nuna wutar lantarki kai tsaye). Yi ƙoƙarin amfani da gajeren baka don walda.


Cikakken Bayani game da Samfurin

Alamun Samfura

Aluminum da Aluminum Alloy Electrode

L109                                                     

GB/T E1100

AWS A5.3 E1100

Bayani: L109 wani tsararren lantarki ne na aluminum wanda ke da rufin gishiri. Yi amfani da DCEP (mai nuna wutar lantarki kai tsaye). Yi ƙoƙarin amfani da gajeren baka don walda.

Aikace-aikace: Ana amfani da shi don walda faranti na aluminum da kwantena na aluminum masu tsabta.

Sinadarin sinadarai na ƙarfen walda(%):

Si+Fe

Cu

Mn

Zn

Al

Wani

≤0.95

0.05 ~ 0.20

≤0.05

≤0.10

≥99.0

≤0.15

 

 

Kayan aikin injiniya na ƙarfe na walda:

Gwaji abu

Ƙarfin tauri

Mpa

An Garanti

≥80

 

 

Shawarar da ake bayarwa:

Diamita na sanda

(mm)

3.2

4.0

5.0

Walda na yanzu

(A)

80 ~ 100

110 ~ 150

150 ~ 200

 

Sanarwa:

1. Na'urar lantarki tana da sauƙin shafar danshi, don haka ya kamata a adana ta a cikin busasshiyar akwati mai hana iska shiga domin hana ta lalacewa saboda danshi; dole ne a gasa na'urar lantarki a kusan 150°C na tsawon awanni 1 zuwa 2 kafin a yi walda;

2. Ya kamata a yi amfani da faranti na baya kafin a yi walda, sannan a yi walda bayan an dumama ta zuwa 200 ~ 300°C gwargwadon kauri na walda; sandar walda ya kamata ta kasance daidai da saman walda, baka ya kamata ya zama gajere gwargwadon iko, kuma a yi maye gurbin sandunan walda da sauri;

3. Dole ne a tsaftace walda da mai da ƙazanta kafin a yi walda, sannan a cire tarkacen a hankali bayan an yi walda, sannan a wanke da tururi ko ruwan zafi.

 

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 