AWS: SFA 5.4 E316-16 Electrodes ɗin Walda na Bakin Karfe

Takaitaccen Bayani:

A201(AWS E316-16) na'urar lantarki ce ta bakin ƙarfe mai ƙarancin carbon Cr18Ni12Mo2 tare da rufin titanium-calcium.


Cikakken Bayani game da Samfurin

Alamun Samfura

Bakin Karfe Walda Electrode

A201                                      

GB/T E316-16

AWS E316-16

Bayani: A201 na'urar lantarki ce ta bakin ƙarfe mai ƙarancin carbon Cr18Ni12Mo2 tare da murfin titanium-calcium. Ana iya amfani da shi don AC da DC tare da kyakkyawan aikin aiki, musamman ya dace da walda mai faɗi da walda na faranti masu sirara. Rufin ba ya yin ja ko fashewa yayin walda. Saboda ƙara molybdenum ga ƙarfe da aka ajiye, yana da kyakkyawan juriya ga tsatsa, juriya ga zafi da juriya ga tsatsa, musamman don juriya ga tsatsa ta ion chloride.

Aikace-aikace: Ana amfani da shi don walda 06Cr17Ni12Mo2 tsarin ƙarfe mai bakin ƙarfe wanda ke aiki a cikin matsakaiciyar acid na halitta da na inorganic (acid mara oxidizing), kuma ana iya amfani da shi don walda ƙarfe mai tsayi ko ƙarfe daban-daban waɗanda ba za a iya magance su da zafi ba bayan walda.

 

 

Sinadarin sinadarai na ƙarfen walda(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.08

0.5 ~ 2.5

≤0.90

17.0 ~ 20.0

11.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Kayan aikin injiniya na ƙarfe na walda:

Gwaji abu

Ƙarfin tauri

Mpa

Ƙarawa

%

An Garanti

≥520

≥30

 

Shawarar da ake bayarwa:

Diamita na sanda

(mm)

2.0

2.5

3.2

4.0

5.0

Walda na Wuta

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Sanarwa:

1. Dole ne a gasa wutar lantarki na tsawon awa 1 a kusan digiri 250 kafin a fara aikin walda. Kada a sake gasa ta akai-akai;

2. Saboda zurfin shigar ciki ba shi da zurfi yayin walda ta AC, ya kamata a yi amfani da wutar lantarki ta DC gwargwadon iyawa don samun zurfafa shigar ciki.

 

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.


  • Na baya:
  • Na gaba: