AWS A5.13/AME A5.13 ECoCr-C LANTARKI MAI TAURARWA

Takaitaccen Bayani:

Tauraron kan bawul mai ƙarfi, zoben hatimin famfo mai matsin lamba da sassan injin niƙa.


Cikakken Bayani game da Samfurin

Alamun Samfura

BAYANI:

Electrode mai rufe COBALTHARD 1FC shine mafi girman ƙarfen da aka saba amfani da shi a cikin rukunin ƙarfen cobalt da ake amfani da shi don lalacewar zafi mai yawa da ke da alaƙa da tsatsa. Ajiyar wannan ƙarfen tana da babban adadin chromium carbide waɗanda ke shafar juriyar tsatsa mai ban mamaki. Ƙara tungsten yana ƙara tauri mai yawa da tauri mai yawa don ingantaccen juriyar mannewa da yashewar barbashi. Yana haɗuwa da kyau da dukkan ƙarfe, gami da bakin ƙarfe.

AIKACE-AIKACE:

Tauraron kan bawul mai ƙarfi, zoben hatimin famfo mai matsin lamba da sassan injin niƙa.

Taurin Ajiya na ƙarfe na walda: 50 – 56 HRC (520- 620 Hv)

ABUBUWAN DA KE CIKI NA KARFE NA WALDA (%):

C Si Mn Cr W Co
2.15 0.47 1.03 31.25 12.72 Bal

MATSAYIN WALDA: LEƘE, A TSAYA, A KAN KAI

GIRMAN DA AKE SAMU DA KWALLON DA AKA SHAWARA (DC +):

Girman (dia. mm) 3.2 4.0 5.0
Tsawon (mm) 350 350 350
Nisan Yanzu (Amp) 90 – 120 110 – 150 140 – 180

BAYANI AKAN AMFANI:

A kunna wuta a 300ºC kuma a sama gaba ɗaya.

Yi amfani da sandunan nuna zafin jiki na PHILARC ko ma'aunin zafin jiki na PHILARC don tantance ko an cimma zafin da ya dace kafin walda.

Yana da tasiri wajen dumamawa a zafin 600ºC da kuma rage sanyi bayan walda don hana fashewa.

Busar da na'urorin lantarki a zafin 150-200ºC na tsawon mintuna 30-60 kafin amfani. Yi amfani da tanda mai busarwa ta PHILARC.