Inganci mai inganci da kuma kyakkyawan matsayin bashi su ne ƙa'idodinmu, waɗanda za su taimaka mana a matsayi mafi girma. Bin ƙa'idar "ingancin farko, mafi girma ga mai siye" don Samar da OEM/ODM 3 * 7mmpp/PE/PVC Plastic Electrode don Walda na filastik, Muna ba da fifiko ga inganci da gamsuwar abokin ciniki kuma don haka muna bin tsauraran matakan kula da inganci. Muna da wuraren gwaji na cikin gida inda ake gwada samfuranmu a kowane fanni a matakan sarrafawa daban-daban. Kasancewar sabbin fasahohi, muna sauƙaƙa wa abokan cinikinmu da kayan aikin samarwa na musamman.
Inganci mai kyau da kuma kyakkyawan matsayin bashi sune ƙa'idodinmu, waɗanda zasu taimaka mana a matsayi mafi girma. Bin ƙa'idar ku ta "ingantaccen inganci na farko, mai siye mafi girma" donSandunan Walda na China da Sandar PolyethyleneKayayyakin da mafita suna da kyakkyawan suna tare da farashi mai kyau, ƙirƙira na musamman, wanda ke jagorantar yanayin masana'antu. Kamfanin ya dage kan manufar ra'ayin cin nasara, ya kafa hanyar sadarwa ta tallace-tallace ta duniya da kuma hanyar sadarwa ta bayan-tallace-tallace.
AIKACE-AIKACE:
Walda na ƙarfe 9% na Cr-1% na Mo da ƙarfe 9% na Cr-2% na Mo da ake amfani da su don wutar lantarki da kuma babban matsin lamba.
BAYANI:
PA-8016-B8 ƙaramin lantarki ne na hydrogen wanda ƙarfen walda ya ƙunshi 9%Cr-1%Mo. An ƙera shi don ƙarfe mai zafi da ƙarfe don ayyukan hydrogen mai zafi, musamman a masana'antar sinadarai na petrochemical. Ana iya amincewa da electrode ɗin saboda ƙarfinsa mai yawa, kyakkyawan tauri da kuma juriyar zafi.
BAYANI AKAN AMFANI:
1. A busar da electrodes ɗin a zafin 350-400°C na kimanin awa ɗaya kafin amfani sannan a adana electrodes ɗin a zafin 100-150°C bayan an busar da su da kulawa don a nisantar da su daga danshi.
2. Yi amfani da hanyar matakan baya ko kuma buga baka a kan ƙaramin farantin ƙarfe da aka shirya don wannan takamaiman dalili don hana busawa a baka fara.
3. A rage girman baka gwargwadon iyawa.
4. A kunna wuta a zafin 100-150°C. Zafin da za a shafa ya bambanta dangane da kauri da kuma irin ƙarfen da za a haɗa.
5. Kula da kada a wuce yadda ya kamata wajen shigar da zafi saboda yawan shigar zafi yana haifar da lalacewar ƙimar tasiri da ƙarfin samar da ƙarfe na walda.
IV. SIMINI NA AL'ADA NA KARFE NA WALDA (%):
| C | Si | Mn | Cr | Mo |
| 0.06 | 0.42 | 0.68 | 9.38 | 1.05 |
V. ABUBUWAN INJI NA AL'ADA NA KARFE MAI WALDA:
| Ƙarfin Tauri N/mm2(Ksi) | Ma'aunin Yawa N/mm2 (Ksi) | Ƙarawa % | PWHT |
| 705 (102) | 560 (81) | 24 | 740°C x awa 1 |
VI. MATSAYIN WALDA: DUKKAN MATSAYI
VII. GIRMA DA JERIN KWANA NA YANZU DA AKA BA DA SHAWARA (AC/DC+):
| Diamita (mm) | 2.5 | 3.2 | 4.0 | 5.0 | |
| Tsawon (mm) | 350 | 350 | 400 | 400 | |
| Ampere | Flat | 55 – 85 | 90 – 130 | 130 – 180 | 180 – 240 |
| V da OH | 50 – 80 | 80 – 115 | 110 – 170 | 150 – 200 |
Inganci mai inganci da kuma kyakkyawan matsayin bashi su ne ƙa'idodinmu, waɗanda za su taimaka mana a matsayi mafi girma. Bin ƙa'idar "ingancin farko, mafi girma ga mai siye" don Samar da OEM/ODM 3 * 7mmpp/PE/PVC Plastic Electrode don Walda na filastik, Muna ba da fifiko ga inganci da gamsuwar abokin ciniki kuma don haka muna bin tsauraran matakan kula da inganci. Muna da wuraren gwaji na cikin gida inda ake gwada samfuranmu a kowane fanni a matakan sarrafawa daban-daban. Kasancewar sabbin fasahohi, muna sauƙaƙa wa abokan cinikinmu da kayan aikin samarwa na musamman.
Samar da OEM/ODMSandunan Walda na China da Sandar PolyethyleneKayayyakin da mafita suna da kyakkyawan suna tare da farashi mai kyau, ƙirƙira na musamman, wanda ke jagorantar yanayin masana'antu. Kamfanin ya dage kan manufar ra'ayin cin nasara, ya kafa hanyar sadarwa ta tallace-tallace ta duniya da kuma hanyar sadarwa ta bayan-tallace-tallace.