Labarai
-
Inganta Walda na Karfe na Carbon tare da Waya ta AWS A5.18 ER70S-6
Wayar walda ta ER70S-6 an san ta da keɓantaccen tsari, wanda ya haɗa da babban sinadarin manganese da silicon. Waɗannan abubuwan suna taka muhimmiyar rawa wajen inganta aikin wayar, musamman lokacin da ake haɗa saman walda waɗanda ba su da kyau. Ko dai ana mu'amala da datti, mai ko tsatsa...Kara karantawa -
Amfani da Waya Mai Juyawa don Ingantaccen Ingancin Walda
An ƙera wayar Flux cored don walda ƙananan ƙarfe marasa carbon waɗanda ke ɗauke da chromium 18-20% da nickel 8-12%. Wannan abun da ke ciki na musamman yana ba da kyakkyawan damar walda, yana tabbatar da cewa masu walda za su iya samun haɗin gwiwa masu ƙarfi da aminci ba tare da ƙarancin ƙoƙari ba. Kasancewar ferrite a cikin ƙarfen walda babban abin tsoro ne...Kara karantawa -
Muhimmin rawar da na'urorin walda ke takawa a cikin aikin aluminum
An ƙera AWS/ASME 5.3 E 4047 Aluminum Welding Electrode a hankali don samar da sakamako mafi kyau a aikace-aikacen walda arc. Tsarinsa na musamman yana ba da damar kwanciyar hankali mai kyau da ƙarancin sptatter, waɗanda sune manyan abubuwan da ke haifar da walda mai tsabta da daidaito. Lokacin walda gami da aluminum, injin...Kara karantawa -
Inganta ayyukan walda da kake yi da AWS A5.11 ENiCrFe-2 Welding Electrode na Nickel Ni307-2
Ana siffanta na'urorin lantarki na Ni307-2 da rufin sodium mai ƙarancin hydrogen, wanda ke taka muhimmiyar rawa wajen rage haɗarin fashewa da hydrogen ke haifarwa. Wannan kadara tana da amfani musamman lokacin aiki da ƙarfe masu ƙarfi da sauran kayan da ke iya fuskantar irin wannan lahani. Ta hanyar amfani da Ni307-...Kara karantawa -
Inganta ayyukan walda da kake yi da na'urorin lantarki na cobalt na ECoCr-B
EcoCr-B cobalt alloy electrodes sun faɗi ƙarƙashin ma'aunin A5.13, wanda ke nuna dacewarsu ga aikace-aikacen shirye-shiryen saman mai ƙarfi. Wannan rarrabuwa yana tabbatar da cewa masu amfani za su iya dogaro da inganci da aikin waɗannan electrodes. Haɗin cobalt alloy yana ba da kyakkyawan juriya ga lalacewa...Kara karantawa -
Mafi kyawun zaɓi don walda: AWS ECuSi ƙarfe mai ƙarfe
An yi na'urar walda ta T207 (AWS ECuSi) da sinadarin silicon tagulla, wanda yake da mahimmanci don samun walda mai ƙarfi da juriya. An ƙera wannan na'urar walda ta tagulla don samar da juriya mai kyau ga tsatsa, kuma ta dace da amfani a cikin mawuyacin yanayi. Ba wai kawai na'urar walda ta tagulla ta silicon tana ƙara...Kara karantawa -
Inganta ayyukan walda da kake yi da na'urorin lantarki masu tauri na DIN 8555 (E6-UM-60)
An ƙera sandunan walda masu tauri na DIN 8555 (E6-UM-60) don biyan buƙatun da suka dace na aikace-aikacen masana'antu daban-daban. Tsarinsa na musamman yana ba da kyakkyawan mannewa da shiga ciki, yana tabbatar da haɗin gwiwa mai ƙarfi tsakanin substrate da walda. Wannan fasalin yana da amfani musamman a cikin...Kara karantawa -
Sauƙin amfani da Ingancin Sandar Walda ta Karfe Mai Ƙarancin Zafi ta W707
An ƙera sandar walda ta W707 don samar da ingantaccen aiki a cikin mawuyacin yanayi. Ƙarfinta mai ƙarancin zafin jiki yana ba da damar walda mai inganci a cikin muhalli inda sandar walda ta gargajiya za ta sha wahala. Wannan fasalin yana da amfani musamman ga masana'antu da ke aiki a cikin yanayin sanyi ko...Kara karantawa -
Fa'idodin Sandunan Walda Masu Ƙarancin Alloy: Duba Zurfi Kan AWS E10015-D2
An ƙera sandar walda mai ƙarancin ƙarfe ta AWS E10015-D2 don aikace-aikacen walda iri-iri, musamman waɗanda ke buƙatar ƙarfi da juriya. Wannan electrode mai ƙarancin ƙarfe an lulluɓe shi da kayan sodium mai ƙarancin hydrogen wanda ke taka muhimmiyar rawa wajen rage haɗarin fashewa da hydrogen ke haifarwa a lokacin...Kara karantawa -
Jagorar Asali ga Electrodes ɗin Walda na ƙarfe: AWS ENiFe-C1 (Z408)
An ƙera na'urar lantarki ta ƙarfe ta AWS ENiFe-C1 (Z408) don samar da kyakkyawan aiki a cikin hanyoyin walda na alternating current (AC) da direct current (DC). Wannan ƙarfin aiki mai amfani biyu yana bawa masu walda damar amfani da na'urar lantarki a wurare daban-daban, ko a shago ko a filin...Kara karantawa -
Mafi kyawun Zaɓuɓɓuka don Walda: 316 Bakin Karfe da AWS A5.4 E316L-16 Electrodes
An yi sandunan walda na AWS A5.4 E316L-16 daga bakin karfe mai ƙarancin carbon Cr18Ni12Mo2, wanda ke inganta aikinsa a fannoni daban-daban na walda. Ƙarancin sinadarin carbon yana rage haɗarin hazo na carbide yayin walda, wanda zai iya haifar da tsatsa tsakanin granular. Wannan fasalin...Kara karantawa -
Fa'idodin amfani da na'urorin lantarki na cellulose a cikin walda: Mayar da hankali kan AWS E6010
Sanda mai walda ta AWS E6010 an san ta da yawan sinadarin cellulose, wanda ke taka muhimmiyar rawa a tsarin walda. Rufin cellulose yana samar da garkuwar iskar gas mai kariya yayin walda, wanda ke taimakawa wajen hana gurɓatawa daga abubuwan da ke cikin yanayi. Wannan fasalin yana da amfani musamman lokacin amfani da...Kara karantawa