Sayarwa Mai Zafi Don Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Carbon Steel Arc Welding Electrode

Takaitaccen Bayani:

J556 (AWS E8016-G) wani lantarki ne mai ƙarancin ƙarfe mai kauri wanda ke da rufin sinadarin hydrogen potassium mai ƙarancin hydrogen. Ana iya amfani da AC da DC duka, kuma ana iya haɗa su a kowane matsayi.


Cikakken Bayani game da Samfurin

Alamun Samfura

Bisa ga ka'idar "inganci, ayyuka, aiki da ci gaba", mun sami amincewa da yabo daga masu siyayya na cikin gida da na duniya don Sayar da Zafi akan Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Carbon Steel Arc Welding Electrode, muna fatan za mu iya samun dangantaka mai kyau da ɗan kasuwa daga ko'ina cikin duniya.
Bisa ga ka'idar "inganci, ayyuka, aiki da ci gaba", mun sami amincewa da yabo daga masu siyayya na cikin gida da na duniya donElectrode na Walda da Walda na China E7018Muna maraba da damar yin kasuwanci da ku kuma muna fatan jin daɗin haɗa ƙarin bayani game da samfuranmu da mafita. Inganci mai kyau, farashi mai gasa, isarwa akan lokaci da kuma sabis mai aminci za a iya tabbatar da shi. Don ƙarin tambayoyi, kada ku yi jinkirin tuntuɓar mu.
AIKACE-AIKACE:

Walda na ƙarfe 9% na Cr-1% na Mo da ƙarfe 9% na Cr-2% na Mo da ake amfani da su don wutar lantarki da kuma babban matsin lamba.

BAYANI:

PA-8016-B8 ƙaramin lantarki ne na hydrogen wanda ƙarfen walda ya ƙunshi 9%Cr-1%Mo. An ƙera shi don ƙarfe mai zafi da ƙarfe don ayyukan hydrogen mai zafi, musamman a masana'antar sinadarai na petrochemical. Ana iya amincewa da electrode ɗin saboda ƙarfinsa mai yawa, kyakkyawan tauri da kuma juriyar zafi.

BAYANI AKAN AMFANI:

1. A busar da electrodes ɗin a zafin 350-400°C na kimanin awa ɗaya kafin amfani sannan a adana electrodes ɗin a zafin 100-150°C bayan an busar da su da kulawa don a nisantar da su daga danshi.

2. Yi amfani da hanyar matakan baya ko kuma buga baka a kan ƙaramin farantin ƙarfe da aka shirya don wannan takamaiman dalili don hana busawa a baka fara.

3. A rage girman baka gwargwadon iyawa.

4. A kunna wuta a zafin 100-150°C. Zafin da za a shafa ya bambanta dangane da kauri da kuma irin ƙarfen da za a haɗa.

5. Kula da kada a wuce yadda ya kamata wajen shigar da zafi saboda yawan shigar zafi yana haifar da lalacewar ƙimar tasiri da ƙarfin samar da ƙarfe na walda.

IV. SIMINI NA AL'ADA NA KARFE NA WALDA (%):

C

Si

Mn

Cr

Mo

0.06

0.42

0.68

9.38

1.05

V. ABUBUWAN INJI NA AL'ADA NA KARFE MAI WALDA:

Ƙarfin Tauri N/mm2(Ksi)

Ma'aunin Yawa N/mm2

(Ksi)

Ƙarawa %

PWHT

705 (102)

560 (81)

24

740°C x awa 1

VI. MATSAYIN WALDA: DUKKAN MATSAYI

VII. GIRMA DA JERIN KWANA NA YANZU DA AKA BA DA SHAWARA (AC/DC+):

Diamita (mm)

2.5

3.2

4.0

5.0

Tsawon (mm)

350

350

400

400

Ampere

Flat

55 – 85

90 – 130

130 – 180

180 – 240

V da OH

50 – 80

80 – 115

110 – 170

150 – 200

Bisa ga ka'idar "inganci, ayyuka, aiki da ci gaba", mun sami amincewa da yabo daga masu siyayya na cikin gida da na duniya don Sayar da Zafi akan Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Carbon Steel Arc Welding Electrode, muna fatan za mu iya samun dangantaka mai kyau da ɗan kasuwa daga ko'ina cikin duniya.
Sayarwa Mai Zafi donElectrode na Walda da Walda na China E7018Muna maraba da damar yin kasuwanci da ku kuma muna fatan jin daɗin haɗa ƙarin bayani game da samfuranmu da mafita. Inganci mai kyau, farashi mai gasa, isarwa akan lokaci da kuma sabis mai aminci za a iya tabbatar da shi. Don ƙarin tambayoyi, kada ku yi jinkirin tuntuɓar mu.


  • Na baya:
  • Na gaba: