ERCuSn-A (Phos Bronze A) Sandunan Tagulla da Tagulla da kuma Electrodes Wayar Tig da Mig

Takaitaccen Bayani:

ERCuSn-A Phos Bronze A tagulla ce ta tagulla mai kama da tagulla wadda ke ɗauke da kusan kashi 5% na tin kuma an ƙara har zuwa kashi 0.35% na phosphorus a matsayin mai cire oxidizer da ake amfani da shi wajen haɗa tagulla da tagulla.


Cikakken Bayani game da Samfurin

Alamun Samfura

ERCuSn-A Phos Bronze A tagulla ce ta tagulla da zinc wadda ke ɗauke da kusan kashi 5% na tin kuma an ƙara har zuwa kashi 0.35% na phosphorus a matsayin mai cire oxidative da ake amfani da shi wajen haɗa tagulla da tagulla. Haka kuma ana iya amfani da shi wajen haɗa tagulla idan kasancewar tin a cikin ƙarfen walda ba abin ƙyama ba ne.

Amfani na yau da kullun: rufe ƙarfe; haɗa ƙarfe mai tushe na ƙarfe mai tagulla da tin 509-519

Ajin AWS: ERCuSn-A Takaddun shaida: AWS A5.7/A5.7M:2007
Na'urar haɗa ƙarfe: ERCuSn-A ASME SFA A5.7

 

Matsayin Walda: Na yanzu:
AC-DCEP

 

Ƙarfin Taurin Kai, kpsi: 35
Taurin Brinell 70-85

Sinadarin Waya na yau da kullun kamar yadda yake a cikin AWS A5.7 (ƙima ɗaya ita ce mafi girma)

Cu ciki har da Ag Al Pb P Sn Wani
Sauran 0.01 0.02 0.10-0.35 4.0-6.0 0.50

 

Sigogi na Walda na yau da kullun
diamita Tsarin aiki Volt Amps GAS
in (mm)
1/16 (1.6) GTAW 70-120 70-150 ACHF ta amfani da 100% Argon ko Helium 2% Thoriated, Ceriated ko Lanthanum Tungsten Electrode
3/32 (2.4) GTAW 120-160 140-230 ACHF ta amfani da 100% Argon ko Helium 2% Thoriated, Ceriated ko Lanthanum Tungsten Electrode
1/8 (3.2) GTAW 170-230 225-320 ACHF ta amfani da 100% Argon ko Helium 2% Thoriated, Ceriated ko Lanthanum Tungsten Electrode
Sigogi na Walda na yau da kullun
diamita Tsarin aiki Volt Amps GAS
in (mm)
0.035 (1.6) GMAW 20-26 100-200 Argon 100% ko 75% Argon, 25% Helium
0.045 (2.4) GMAW 22-28 100-250 Argon 100% ko 75% Argon, 25% Helium
1/16 (3.2) GMAW 29-32 250-400 Argon 100% ko 75% argon, 25% Helium
3/32 (3.2) GMAW 32-34 350-500 Argon 100% ko 75% Argon, 25% Helium

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 

 

 

 