ER5356 wani ƙarfe ne na aluminum wanda aka yi amfani da shi a matsayin ƙarfe na gama gari wanda galibi ana zaɓarsa saboda ƙarfinsa mai yawa. Bugu da ƙari, yana kuma ba da kyakkyawan juriya ga tsatsa idan aka fallasa shi ga ruwan gishiri. Ya kamata a yi la'akari da ER5356 don walda ƙarfe masu tushe na aluminum na jerin 5000.
Aikace-aikace na yau da kullun: waya mai cike walda
| Ajin AWS: ER5356 | Takaddun shaida: AWS A5.10/ A5.10M:1999 |
| Na'urar haɗa ƙarfe: ER5356 | AWS/ASME SFA A5.10 |
| Matsayin Walda: F, V, OH, H | Na yanzu: DCEP-GMAW AC-GTAW |
| Gudanar da wutar lantarki: | 29% IACS (-0)/27% IACS (-H18) |
| Ƙarfin Taurin Kai, kpsi: | 38 |
| Launi: | Fari |
| Wurin narkewa | 1175⁰F | Ƙarfafawa | 1060⁰F | Yawan yawa | 0.096 lbs/cu In. |
| Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | Wani | AL |
| 0.25 | 0.40 | 0.10 | 0.50-1.0 | 4.7-5.5 | 0.05-0.20 | 0.25 | 0.05-0.20 | 0.15 | Sauran |
| Sigogi na Walda na yau da kullun | |||||
| diamita | Tsarin aiki | Volt | Amps | GAS | |
| in | (mm) | ||||
| .030 | (.8) | GMAW | 15-24 | 60-175 | Argon (cfh) |
| .035 | (.9) | GMAW | 15-27 | 70-185 | Argon (cfh) |
| 3/64” | (1.2) | GMAW | 20-29 | 125-260 | Argon (cfh) |
| 1/16” | (1.6) | GMAW | 24-30 | 170-300 | Argon (cfh) |
| 3/32” | (2.4) | GMAW | 26-31 | 275-400 | Argon (cfh) |
| diamita | Tsarin aiki | Volt | Amps | GAS | |
| in | (mm) | ||||
| 1/16” | (1.6) | GTAW | 15 | 60-80 | Argon (cfh) |
| 3/32” | (2.4) | GTAW | 15 | 125-160 | Argon (cfh) |
| 1/8” | (3.2) | GTAW | 15 | 190-220 | Argon (cfh) |
| 5/32” | (4.0) | GTAW | 15 | 200-300 | Argon (cfh) |
| 3/16” | (4.8) | GTAW | 15-20 | 330-380 | Argon (cfh) |
An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.
Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.