ER1100 A5.10, Electrodes da sandunan Aluminum da Aluminum
ER1100 yana da juriya sosai ga hare-haren sinadarai da kuma yanayin yanayi. Gashi ne mai laushi wanda yake da sauƙin ƙirƙira kuma ana amfani da shi sosai a cikin samfuran ma'aunin sirara da foil. Yana da kyawawan halaye na jika kuma ana amfani da shi azaman gamin cikawa don dalilai na walda. Wani siffa mai kyau na gamin shine ƙarewa mai haske da aka samu ta hanyar anodizing.
Aikace-aikace na yau da kullun: musayar zafi; kayan aikin sarrafa abinci; rivets; waya ta ɗaure; ƙara ƙarfe
| Ajin AWS: ER1100 | Takaddun shaida: AWS A5.10/ A5.10M:1999 |
| Na'urar haɗa ƙarfe: ER1100 | AWS/ASME SFA A5.10 |
| Matsayin Walda: F, V, OH, H | Na yanzu: DCEP-GMAW AC-GTAW |
Al'ada Properties (kamar yadda aka welded)
| Gudanar da wutar lantarki: | 59% IACS (-12) |
| Ƙarfin Taurin Kai, kpsi: | 13 |
| Launi: | Toka-toka |
| Wurin narkewa | 1215⁰F | Ƙarfafawa | 1090⁰F | Yawan yawa | 0.098 lbs/cu In. |
Sinadarin Waya na yau da kullun kamar yadda yake a cikin AWS A5.10 (ƙima ɗaya ita ce mafi girma)
| Si + Fe | Cu | Mn | Zn | Wani | Al | ||||||
| 0.95 | 0.05-0.20 | 0.05 | 0.10 | 0.15 | Minti 99.0 | ||||||
| Sigogi na Walda na yau da kullun | |||||||||||
| diamita | Tsarin aiki | Volt | Amps | GAS | |||||||
| in | (mm) | ||||||||||
| .030 | (.8) | GMAW | 15-24 | 60-175 | Argon (cfh) | ||||||
| .035 | (.9) | GMAW | 15-27 | 70-185 | Argon (cfh) | ||||||
| 3/64” | (1.2) | GMAW | 20-29 | 125-260 | Argon (cfh) | ||||||
| 1/16” | (1.6) | GMAW | 24-30 | 170-300 | Argon (cfh) | ||||||
| 3/32” | (2.4) | GMAW | 26-31 | 275-400 | Argon (cfh) | ||||||
| diamita | Tsarin aiki | Volt | Amps | GAS | |||||||
| in | (mm) | ||||||||||
| 1/16” | (1.6) | GTAW | 15 | 60-80 | Argon (cfh) | ||||||
| 3/32” | (2.4) | GTAW | 15 | 125-160 | Argon (cfh) | ||||||
| 1/8” | (3.2) | GTAW | 15 | 190-220 | Argon (cfh) | ||||||
| 5/32” | (4.0) | GTAW | 15 | 200-300 | Argon (cfh) | ||||||
| 3/16” | (4.8) | GTAW | 15-20 | 330-380 | Argon (cfh) | ||||||
An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.
Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.