E70C-6M Carbon Karfe Flux Cored Arc Welding Electrodes Flux Core Welding Waya

Takaitaccen Bayani:

Wayar walda mai kauri ta E70C-6M tana haɗa ingancin wayoyi masu ƙarfi (GMAW) tare da yawan samar da wayoyi masu ƙarfi (FCAW) - ƙarancin samar da hayaki, inganci mai yawa, babu slag don tsaftacewa ko cirewa - tare da duk fa'idodin da wayoyi masu kauri ke da su akan wayoyi masu ƙarfi - babu "sanyi" ko rashin haɗakar gefe, nasarar feshi mai tsabta tare da argon/balance carbon dioxide 75-80%, saurin tafiya mai sauri don girman fillet ɗin da aka bayar.


Cikakken Bayani game da Samfurin

Alamun Samfura

Wayar walda mai kauri ta E70C-6M tana haɗa ingancin wayoyi masu ƙarfi (GMAW) tare da yawan samar da wayoyi masu ƙarfi (FCAW) - ƙarancin yawan samar da hayaki, inganci mai yawa, babu slag don tsaftacewa ko cirewa - tare da duk fa'idodin da wayoyi masu kauri ke da su akan wayoyi masu ƙarfi - babu "sanyi" ko rashin haɗakar gefe, nasarar feshi mai tsabta tare da argon/balance carbon dioxide 75-80%, saurin tafiya mai sauri don girman fillet. E70C-6M ya dace da aikace-aikace inda matakan manganese da silicon suka fi mahimmanci, kamar a gaban ma'aunin niƙa mai nauyi ko gurɓatattun abubuwa masu sauƙi, ko lokacin da ake son a sami isasshen jika na bead ɗin walda. Wannan samfurin ya fi kyau a walda gabaɗaya, amma ya fi kyau a cikin yanayi mafi girma kamar a cikin ƙera ƙarfe mai nauyi, aikin gini, walda bututu da walda na masu dumama ruwan zafi.

Ajin AWS: E70C-6M Takaddun shaida: AWS A5.18/A5.18M:2005
Na'urar Gami: E70C-6M ASME SFA A5.18

 

Matsayin Walda: F, H, V, OH .035-1/16”
F, H 5/64”-1/8”
Na yanzu:
DCEP

 

Ƙarfin Taurin Kai, kpsi: 70 100% CO2
Ƙarfin Samar da Aiki, kpsi: 58 100% CO2
Ƙarawa a cikin 2"%: 22 100% CO2

Sinadarin Waya na yau da kullun kamar yadda yake a cikin AWS A5.18 (ƙima ɗaya ita ce mafi girma)

C Mn Si S P Ni Cr Mo V Cu  
0.12 1.75 0.90 0.03 0.03 0.50 0.20 0.30 0.08 0.50  
Sigogi na Walda na yau da kullun
diamita Tsarin aiki Volt Amps Iskar Gas Mai Kariya
in (mm)
.035 (0.9) GMAW 24-35 160-250 75-95% Ar/balance Co2, 35-50cfh
.045 (1.2) GMAW 37-33 180-330 75-95% Ar/balance Co2, 35-50cfh
.052 (1.3) GMAW 25-35 220-460 75-95% Ar/balance Co2, 35-50cfh
1/16 (1.6) GMAW 26-37 240-520 75-95% Ar/balance Co2, 35-50cfh
5/64 (2) GMAW 27-36 240-550 75-95% Ar/balance Co2, 35-50cfh
3/32 (2.4) GMAW 28-36 350-550 75-95% Ar/balance Co2, 35-50cfh
7/64 (2.78) GMAW 27-34 400-600 75-95% Ar/balance Co2, 35-50cfh
1/8 (3.2) GMAW 26-32 95-145 75-95% Ar/balance Co2, 35-50cfh

 

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun kasance muna ƙera na'urorin walda,sandunan walda, da kuma kayan aikin walda na tsawon shekaru sama da 20.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.


  • Na baya:
  • Na gaba: