Wayar Walda ta Tagulla ta AWS ERCU

Takaitaccen Bayani:

ERCu wani ƙarfe ne na tagulla wanda aka haɓaka don samar da ma'adanai masu yawa, masu inganci tare da ƙarfin lantarki mai yawa don amfani wajen haɗawa da kuma rufe hanyoyin iskar gas mara aiki.


Cikakken Bayani game da Samfurin

Alamun Samfura

ERCu wani ƙarfe ne na tagulla wanda aka haɓaka don samar da ma'adanai masu yawa, masu inganci tare da ƙarfin lantarki mai yawa don amfani wajen haɗawa da kuma rufe hanyoyin iskar gas mara aiki.
Ana amfani da sandar ƙarfe mai kauri da kuma sandar cika ƙarfe ta ERCu musamman don ƙera jan ƙarfe mai kauri da kuma gyara simintin jan ƙarfe na walda tare da tsarin ƙarfe-arc da gas tungsten-arc. Haka kuma ana iya amfani da shi don walda ƙarfe mai kauri da kuma jan ƙarfe mai kauri zuwa ƙarfe mai laushi inda ba a buƙatar haɗin gwiwa mai ƙarfi.
Ana amfani da wayar ERCu mai tsini da sandar ƙarfe don rufe saman don hana tsatsa. Yawanci ana amfani da ERCu don molds na billet, na'urorin juyawa, abubuwan dumama, sassaka na tagulla, masu riƙe da wutar lantarki na injin niƙa ƙarfe, sandunan bas, da haɗin jan ƙarfe.

Ayyukan jiki da halayen inji:
Yawan digiri 1020 na C 8.9kg/dm Matsakaicin tsawaitawa na 30-40%
Ƙarfin tururin ruwa mai ƙarfi 1050 DEG C 210-220N/mm2, Taurin Brinell 60HB

ERCU ERCU ERCU GELIN WADI NA KERA GERA

Haɗaɗɗen Sinadarai (%)
Ma'auni ISO 24373 GB/T9460 BS EN14640 AWS A5.7 DIN1733
Aji LAMBAR. Cu1898 SCu1898 Cu1898 C18980 2,1006
Alloy NO. CuSn1 CuSn1 CuSn1 ERCu SG-CuSn
Cu Minti 98 Min98 Bal. Minti 98 Bal.
Al 0.01 Matsakaicin 0.01 0.01 0.01 Matsakaicin 0.01
Fe – – 0.05 0.50 Matsakaicin 0.05
Mn 0.50 Matsakaicin 0.5 0.1~0.5 0.50 0.1~0.5
Ni – – 0.3 – Matsakaicin 0.3
P 0.15 Matsakaicin 0.15 0.02 0.15 Matsakaicin 0.02
Pb 0.02 Matsakaicin 0.02 0.02 0.02 Matsakaicin 0.01
Si 0.5 Matsakaicin 0.5 0.5 0.5 0.1~0.5
Sn 1.0 Matsakaicin 1.0 0.5~1.0 1.0 0.5~1.0
As – – 0.05 – Matsakaicin 0.05
Sauran Jimilla 0.5 Matsakaicin 0.5 0.1 0.5 Matsakaicin 0.1

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun shafe sama da shekaru 20 muna kera na'urorin lantarki na walda, sandunan walda, da kuma kayan da ake amfani da su wajen walda.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 

 

 

 


  • Na baya:
  • Na gaba: