Sandunan Walda na AWS E6011

Takaitaccen Bayani:

Na'urar walda ta AWS E6011 nau'in sinadarin cellulose potassium ne, wanda ake amfani da shi don walda a tsaye. Dukansu don walda ta AC da DC.


Cikakken Bayani game da Samfurin

Alamun Samfura

AWS E6011na'urar waldaNau'in sinadarin cellulose potassium ne, wanda ake amfani da shi don walda a tsaye. Dukansu don walda AC da DC. Yana ɗaukar fasahar waje mai ci gaba kuma yana da kyawawan halayen fasaha na walda. Ya kamata a sarrafa tsawon ARC a cikin iyaka mai dacewa. Ba walda mai laushi da murfin da ya dace ba ne.

Aikace-aikace

Sandunan walda AWS E6011 ya dace da tsarin tasoshin walda kamar gine-gine da gadoji, tankunan ajiya, bututu da kayan haɗin matsi.

SIFFOFI:

Ingantaccen farawa cikin sauri

Mafi kyawun arc drive

Slag yana cirewa cikin sauƙi

KYAKKYAWAN AMFANI DA JIKA-JIKA:

Mai sauƙin ɗaukar hoto, mai dacewa don ɗaurewa

Kyakkyawan shigar ciki

Tsaftacewa cikin sauri

Santsi bayyanar beads, yana rage sanyin gwiwa da yankewa ƙasa

IRIN HALITTA: Direct Current Electrode Positive (DCEP) ko AC

DABARUKAN WALDA DA AKA SHAWARA:

Tsawon Baka - Matsakaicin tsayi (1/8" zuwa 1/4")

Faɗi - Ka kasance a gaban kududdufi kuma ka yi amfani da ɗan motsi na bulala

Kwance - Elektrode mai kusurwa kaɗan zuwa saman farantin

Tsaye a Sama - Ƙaramin bulala ko dabarar saƙa

Tsaye Ƙasa - Yi amfani da ƙarfin amperage mai girma da kuma tafiya cikin sauri, kasancewa a gaba da kududdufi

Sama - Ka kasance a gaban kududdufi kuma ka yi amfani da ɗan motsi na bulala

Sinadaran da ke cikinsa (%)

C Mn Si S P
<0.12 0.3-0.6 <0.2 <0.035 <0.04

Kayayyakin Inji na Karfe da aka Ajiye

Kayan Gwaji

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0℃

Darajar Garanti

≥460

≥330

≥16

≥47

Sakamako na Gabaɗaya

485

380

28.5

86

Na'urar Haɓakawa (DC)

diamita

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40 ~ 70

50 ~ 90

90 ~ 130

130 ~ 210

170 ~ 230

Hankali:

1. Yana da sauƙin fallasa ga danshi, don Allah a ajiye shi a cikin yanayin bushewa.

2. Yana buƙatar dumamawa lokacin da fakitin ya karye ko kuma danshi ya sha, zafin dumama ya kamata ya kasance tsakanin 70C zuwa 80C, lokacin dumama ya kamata ya kasance daga awa 0.5 zuwa 1.

3. Lokacin amfani da na'urorin walda masu ƙarfin 5.0mm, ya fi kyau a yi amfani da ƙarfin lantarki mai ƙarfi, mai ƙarancin wutar lantarki, domin inganta aikin walda.