A312 (AWS E309Mo-16) na'urar lantarki ce ta Cr23Ni13Mo2 mai rufin calcium na titanium.


Cikakken Bayani game da Samfurin

Alamun Samfura

Walda Bakin KarfeElektrode

A312                                     

GB/T E309Mo-16

AWS A5.4 E309Mo-16

Bayani: A312 na'urar lantarki ce ta bakin ƙarfe ta Cr23Ni13Mo2 mai rufin calcium na titanium. Ana iya amfani da shi don AC da DC tare da kyakkyawan aikin aiki. Yana da juriya ga tsatsa, tsagewa, da iskar shaka fiye da A302 saboda ƙarfe da aka ajiye yana ɗauke da molybdenum.

Aikace-aikace: Ana amfani da shi don walda irin wannan akwati na bakin karfe mai jure tsatsa daga sinadarin sulfuric acid (ammonia sulfide), kuma ana iya amfani da shi don walda rufin bakin karfe, farantin karfe mai rufi da ƙarfe daban-daban.

 

Sinadarin sinadarai na ƙarfen walda(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.12

0.5 ~ 2.5

≤0.90

22.0 ~ 25.0

12.0 ~ 14.0

2.0 ~ 3.0

≤0.75

≤0.030

≤0.040

 

Kayan aikin injiniya na ƙarfe na walda:

Gwaji abu

Ƙarfin tauri

Mpa

Ƙarawa

%

An Garanti

≥550

≥25

 

Shawarar da ake bayarwa:

Diamita na sanda

(mm)

2.0

2.5

3.2

4.0

5.0

Walda na Wuta

(A)

25 ~ 50

50 ~ 80

80 ~ 110

110 ~ 160

160 ~ 200

 

Sanarwa:

  1. Dole ne a gasa wutar lantarki na tsawon awa 1 a kusan 150℃ kafin a fara aikin walda;
  2. Saboda zurfin shigar ciki ba shi da zurfi yayin walda ta AC, ya kamata a yi amfani da wutar lantarki ta DC gwargwadon iyawa don samun zurfin shigar ciki. Kuma kada wutar ta yi girma sosai don guje wa jajayen sandar walda.

 

 

An kafa kamfanin Wenzhou Tianyu Electronic Co., Ltd. a shekara ta 2000. Mun kasance muna ƙera na'urorin walda,sandunan walda, kumaabubuwan da ake amfani da su na waldasama da shekaru 20.

Manyan kayayyakinmu sun haɗa da na'urorin walda na bakin karfe, na'urorin walda na ƙarfe na carbon, na'urorin walda na ƙarancin alloy, na'urorin walda na saman, na'urorin walda na nickel & cobalt, na'urorin walda masu laushi da ƙarancin alloy, na'urorin walda na bakin karfe, na'urorin walda masu kariya daga iskar gas, na'urorin walda na aluminum, na'urorin walda na arc da ke ƙarƙashin ruwa, na'urorin walda na nickel & cobalt, na'urorin walda na tagulla, na'urorin walda na TIG & MIG, na'urorin walda na tungsten, na'urorin walda na carbon, da sauran kayan haɗin walda da abubuwan amfani.

 


  • Na baya:
  • Na gaba: